Long-term Performance of Silica Fume Concretes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Long-term Performance of Silica Fume Concretes

Author(s): M. Lachemi, G. Li, A. Tagnit-hamou, and P.-c. Aitcin

Publication: Concrete International

Volume: 20

Issue: 1

Appears on pages(s): 59-65

Keywords: chlorides; compressive strength; concretes; durability; elastic modulus; microstructure; silica fume;

DOI:

Date: 1/1/1998

Abstract:
In 1980, a sidewalk was built using 11 different concrete mixes containing varying amounts of cement and silica fume. A part of this experimental sidewalk, made up of four different silica fume concrete mixes, is still in use 16 years later. The sidewalk has been cored to evaluate the long-term performance of silica fume concrete. The long-term behavior of a non-silica fume concrete, placed at the same time, has also been studied. Cores with 95-mm diameter were taken and tested for compressive strength, elastic modulus, spacing factor, and chloride-ion permeability. Moreover, the microstructure of these concretes was observed through a scanning electron microscope. The results obtained show that the silica fume concretes are performing quite satisfactorily and much better than the non-silica fume concrete, given the severe environmental conditions to which they have been exposed.