Ductility of Plain and Confined Concrete Under Different Strain Rates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ductility of Plain and Confined Concrete Under Different Strain Rates

Author(s): W.H. Dilger, R. Koch, and R. Kowalczyk

Publication: Journal Proceedings

Volume: 81

Issue: 1

Appears on pages(s): 73-81

Keywords: confined concrete; ductility; loads (forces); plain concrete; reinforcing steels; strains; stress-strain diagram.

DOI: 10.14359/10649

Date: 1/1/1984

Abstract:
Results of test on plain and confined concrete prisms subjected to different strain rates are presented. The tests show that the predominant effect of tranverse reinforcement is an increased strain under maximum stress and slope of the descending branch of the stress-strain curve. High loading rates increased strength but did not have a pronounced effect on shape of the stress-strain curve.