Structural Concrete Incorporating High Volume of Fly Ash

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Structural Concrete Incorporating High Volume of Fly Ash

Author(s): D. Galeota, M. M. Giammatteo, and R. Marino

Publication: Symposium Paper

Volume: 153

Issue:

Appears on pages(s): 25-42

Keywords: bonding; compressive strength; drying shrinkage; durability; flexural strength; fly ash; fracture properties; freeze thaw durability; modulus of elasticity; splitting tensile strength; strength; Materials Research

DOI: 10.14359/1062

Date: 6/1/1995

Abstract:
The purpose of this study was to examine the mechanical and durability properties of high-volume fly ash concretes for structural applications. Four concrete mixtures were prepared with the amount of fly ash, from Italian source, varying from 0 to 50 percent by weight of total cementitious materials. A large number of concrete specimens were cast and tested to determine the compressive, flexural, and splitting tensile strengths, modulus of elasticity, fracture parameters, concrete-steel bond properties, drying shrinkage, and durability properties. The results of this study showed that high-volume fly ash concrete has considerable potential in a wide variety of structural applications.