Evaluation of Procedures for In Situ Tensile Bond Testing of Concrete Repairs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of Procedures for In Situ Tensile Bond Testing of Concrete Repairs

Author(s): J. E. McDonald and A. M. Vaysburd

Publication: Symposium Paper

Volume: 200

Issue:

Appears on pages(s): 113-130

Keywords: bond; concrete repair; pull-off tests; tensile bond strength; test methods

DOI: 10.14359/10575

Date: 6/1/2001

Abstract:
achieve durable repairs, it is usually necessary to ensure adequate bond between the repair and the existing concrete substrate. Tensile bond tests are being increasingly used for quality control/quality assurance testing. However, there has been little standardization of test methods. Consequently, a total of 266 partial-depth cores in 77 experimental repairs were tested to evaluate the effect of material properties and environmental conditions on the bond between nine repair materials and a common concrete substrate. Three pull-off testing devices were used to determine bond strengths for each of the experimental repairs. In addition, the testing devices themselves were evaluated by analyzing the magnitude and relative precision of the pull-off strengths, modes of failure, and ease of use in an effort to identify a reliable and practical device for determining in situ tensile bond. The optimum depth of core drilling into the existing substrate was determined by comparing theoretical finite element analyses of failure stress and location with measured test results.