Investigations on the Flexural Behavior of Reinforced Concrete Beams Containing Supplementary Cementitious Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Investigations on the Flexural Behavior of Reinforced Concrete Beams Containing Supplementary Cementitious Materials

Author(s): S. Gopalakrishnan, K. Balasubramanian, T. S. Krishnamoorthy, and B. H. Bharatkumar

Publication: Symposium Paper

Volume: 199

Issue:

Appears on pages(s): 645-664

Keywords: cement replacement materials; flexural behavior; fly ash; ground granulated blast furnace slag; high-performance concrete; reinforced concrete; supplementary cementitious materials

DOI: 10.14359/10540

Date: 6/1/2001

Abstract:
It is now established that the incorporation of industrial byproducts, such as fly ash (FA), ground granulated blast furnace slag (GGBFS) and silica fume (SF), in concrete mixtures as partial cement replacement materials (CRMs) significantly enhances the durability related properties of concrete, besides improving its mechanical properties.. Such concretes are termed as High Performance Concretes (HPCs). In HPC mixtures, it is possible to have low W/C with reduced cement content by judicious choice of mineral and chemical admixtures. The assessment of the flexural behavior of reinforced HPC beams is a subject of ongoing research. Standards and codes of practice differ in the definition of compressive stress block parameters of reinforced HPC beams. Hence, investigations were undertaken at the Structural Engineering Research Centre (SERC), Chennai, to investigate the behavior of reinforced HPC beams under flexural loading. The beam specimens for the test programme were designed as under reinforced, balanced and over reinforced sections as per the guidelines given in the Indian code of practice for reinforced concrete, IS:451 978. The influence of supplementary cementitious materials (SCMs) used as cement replacement materials (CRMs), viz., fly ash (25% as CRM) and GGBFS (40% as CRM), on the flexural behavior of reinforced HPC beams was studied. The paper presents the details of the investigations and discusses the results obtained.