Title: Creep of Fly Ash Concrete

Author(s): Ram S. Ghosh and John Timusk

Publication: Journal Proceedings

Volume: 78

Issue: 5

Appears on pages(s): 351-357

Keywords: cement types; compressive strength; concretes; creep properties; fly ash; modulus of elasticity; shrinkage.

DOI: 10.14359/10519

Date: 9/1/1981

Abstract:
The effect of different qualities of fly ash and different ash to cement ratios on creep, shrinkage, and modulus of elasticity for concretes with 20 MPa (3aK) psi) and 55 MPa (8000 psi) compressive strengths was determined. Results were compared with those for reference concretes of equal workability and 3- or 28-day strengths. Compared to reference concretes, it was found that concretes using fly ash of good quality had equivalent modulus of elasticity value and significantly lower creep and shrinkage. When borderline fly ash was used, the above properties were of comparable magnitude.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer