Flexural Behavior of Hybrid Fiber-Reinforced Cement Composites Containing High-Volume Fly Ash

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Flexural Behavior of Hybrid Fiber-Reinforced Cement Composites Containing High-Volume Fly Ash

Author(s): N. Ramanalingam, P. Paramasivam, M. A. Mansur, and M. Maalej

Publication: Symposium Paper

Volume: 199

Issue:

Appears on pages(s): 147-162

Keywords: cementitious composites; compressive strength; fiber reinforced; flexural strength; fly ash

DOI: 10.14359/10490

Date: 6/1/2001

Abstract:
In recent years, there has been a growing interest in the development of thin walled fiber reinforced cement composites for structural applications. In these composites, the discrete fibers used may be made of metallic, mineral, polymeric or naturally occurring materials. Each type of fibers is unique in geometrical shape, size, surface characteristics, strength, stiffness and ductility. As a result, different fibers offer different extent of improvement to the matrix mechanical properties. However, the most sought-after property in a cement-based composite is the strain-hardening response that is associated with multiple cracking. In order to achieve this property, different types of fibers may be suitably combined to exploit their unique properties. In addition, partial replacement of cement by fly ash which has much finer particles than ordinary cement, is likely to modify the properties of the composite by reducing the matrix fracture toughness and enhancing the interfacial bond strength between the fiber and the matrix, thus promoting a strain-hardening response of the composite material. It would also support the recent emphasis on environmental awareness by reducing the cement content in the composite. The present investigation is therefore undertaken with the main objective of developing a strain-hardening composite using hybrid fibers and high volume fly ash.