Strength and Durability of Concretes with Slag-Fly Ash-Portland Cement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength and Durability of Concretes with Slag-Fly Ash-Portland Cement

Author(s): A. Borsoi, S. Collepardi, L. Coppola, R. Troli, and M. Collepardi

Publication: Symposium Paper

Volume: 199

Issue:

Appears on pages(s): 115-126

Keywords: carbonation; chloride penetration; composite cement; compressive strength; fly ash; slump; slump loss; slag superplasti-cizer

DOI: 10.14359/10487

Date: 6/1/2001

Abstract:
Composite cements containing portland cement (50%), fly ash (25%) and slag (25%), all interground at a Blaine fineness of about 400 or 500 m2/kg, were produced. Super-plasticized concretes with a slump of 200-230 mm were manufactured by using sulfonated naphthalene (SN) or acrylic polymer (AP). The dosage of super-plasticizers was a little higher (10% more) when finer cements were used. The AP superplasticizer was more effective than that based on SN in terms of lower dosage (20% less) and lower water-cementitious material ratio (10% less) at equal workability. Consequently, higher compressive strength were obtained for concretes with the AP admixture rather than with the N S superplasticizer. The better performance of the AP superplasticizer with respect to the SN admixture was independent of the curing temperature (5 or 20) at early (1 day) and later ages (28-90 days). All the concrete mixtures perform very well for the durability behavior in terms of lower CO2 penetration and chloride diffusion. However, due to the lower water-cementitious material ratio (0.29 vs. 0.32) concretes with the acrylic polymer are potentially more durable than those with the naphthalene-based superplasticizer.