349-01/349R-01: Code Requirements for Nuclear Safety Related Concrete Structures & Commentary

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 349-01/349R-01: Code Requirements for Nuclear Safety Related Concrete Structures & Commentary

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 134

Keywords: admixtures; aggregates; anchorage (structural); beam-column frame; beams (supports); building codes; cements; cold weather construction; columns (supports); combined stress; composite construction (concrete and steel).

DOI:

Date: 2/1/2001

Abstract:

Note: A newer version of this document exists. This document was replaced by 349-06.

This standard covers the proper design and construction of concrete structures which form part of a nuclear power plant and which have nuclear safety related functions, but does not cover concrete reactor vessels and concrete containment structures (as defined by ACI-ASME Committee 359). The structures covered by the Code include concrete structures inside and outside the containment system. This Code may be referenced and applied subject to agreement between the Owner and the Regulatory Authority. The format of this Code is based on the "Building Code Requirement for Structural Concrete (ACI 318-95)" and incorporates recent revisions of that standard, except for Chapter 12, which is based on ACI 318-99.