Title: Ultimate Flexural Capacity of Cracked Polygonal Concrete Sections under Biaxial Bending

Author(s): Troels Brondum-Nielsen

Publication: Journal Proceedings

Volume: 82

Issue: 6

Appears on pages(s): 863-869

Keywords: axial loads; bending; biaxial loads; computer programs; cracking (fracturing); flexural strength; limit state design; partial prestressing; prestressed concrete; prestressing; reinforced concrete; strains; structural analysis.

DOI: 10.14359/10407

Date: 11/1/1985

Abstract:
A method of calculating the ultimate flexural capacity of cracked, fully prestressed, partially prestressed, and nonprestressed arbitrary polygonal concrete sections under biaxial bending is presented. The cross section can be reinforced with any combination of prestressed and nonprestressed reinforcement with individual mechanical properties. The method covers symmetrical and unsymmetrical cross sections and cross sections with polygonal holes. The method is suitable for programmable hand-held calculators.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer