Tensile and Flexural Behavior of Joints in Ferrocement Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Tensile and Flexural Behavior of Joints in Ferrocement Construction

Author(s): P. Paramasivam and M. A. Mansur

Publication: Journal Proceedings

Volume: 82

Issue: 5

Appears on pages(s): 710-715

Keywords: crack width and spacing; ductility; ferrocement; flexural strength;1,. joints (junctions); lap connections; mortars (materials); splicing; strength; ten-sile strength; welded wire fabric.

DOI: 10.14359/10382

Date: 9/1/1985

Abstract:
An investigation into various types of joints that frequently occur in ferrocement construction is reported in this paper. Four different types of joints have been identified and an experimental program was carried out to study the tensile and flexural behavior of these joints. The results of this study are presented and discussed with respect to the cracking characteristics, ductility, and ultimate strength.