Ultimate Capacity of Reinforced Concrete Members of Hollow Circular Sections Subjected to Monotonic and Cyclic Bending

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ultimate Capacity of Reinforced Concrete Members of Hollow Circular Sections Subjected to Monotonic and Cyclic Bending

Author(s): Zamil A. R. Mokrin and Wadi S. Rumman

Publication: Journal Proceedings

Volume: 82

Issue: 5

Appears on pages(s): 653-656

Keywords: axial loads; beam (supports); bending; chimneys; cracking (fractur-ing);cyclic loads; loads (forces); reinforced concrete; stiffness; strength; y i e l d strength.

DOI: 10.14359/10375

Date: 9/1/1985

Abstract:
Experimental investigations were made to determine the ultimate capacity of reinforced concrete members of hollow circular sections subjected to both transverse and axial loads. Of the eight specimens tested, four were monotonically loaded to failure and the other four identical specimens were cyclically loaded before being loaded to failure. All specimens were tested in the presence of an axial load. Specimens differed in the value of the axial load, the amount of longitudinal steel, and the method of loading. The effects of the axial load, the steel ratio, and the method of loading on the strength and stiffness were investigated.




  