Quality Assurance Systems for Concrete Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Quality Assurance Systems for Concrete Construction

Author(s): ACI Committee 121

Publication: Journal Proceedings

Volume: 82

Issue: 4

Appears on pages(s): 537-543

Keywords: acceptability; evaluation; concrete construction; inspection; quality assurance; quality control; structural design.

DOI: 10.14359/10367

Date: 7/1/1985

Abstract:
This paper gives guidance for the development of a quality assurance system for both large and small concrete construction projects. The system involves the identification of quality objectives and their incarporation into a quality assurance plan which is implemented by project organizations through quality assurance programs. The system, as herein defined, is intended to permit the user latitude in judgment with respect to the owner’s needs, the defined quality goals, the importance of the project, the project size and complexity, and the skills of the involved project organizations.