Softening Response of Plain Concrete in Direct Tension

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Softening Response of Plain Concrete in Direct Tension

Author(s): V. S. Gopalaratnam and Surendra P. Shah

Publication: Journal Proceedings

Volume: 82

Issue: 3

Appears on pages(s): 310-323

Keywords: cracking (fracturing); crack width and spacing; cyclic loads; defor-mation; finite element method; mechanical properties; microcracking; plain concrete; serviceability; stiffness; stress-strain relationships; tensile strength;tension.

DOI: 10.14359/10338

Date: 5/1/1985

Abstract:
For rational and accurate analysis of concrete structures, it is often desirable to include the post-cracking resistance of concrete. Due to the difficulties of testing concrete in direct uniaxial tension, only limited and often conflicting data are available. In the present investigation a method was developed to obtain reliable load-deformation behavior in tension, including the post-peak softening response. To characterize the softening response, strains at various locations on the specimens, elongations for various gage lengths, and optical measurements of crack widths were made. Seven different mix proportions were used to obtain information on the influence of aggregate size, water-cement ratio, and volume content of aggregates. An analytical expression has been developed to describe the entire tensile response of concrete.