Guide for Design of Foundations and Shoulders for Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Guide for Design of Foundations and Shoulders for Concrete Pavements

Author(s): ACI Committee 325

Publication: Journal Proceedings

Volume: 82

Issue: 3

Appears on pages(s): 258-265

Keywords: airports; cement-treated soils; concrete pavements; drainage; foun-dations; freezing; highways; moisture content; pavements; pumping; shoul-ders; soil cement; soil compacting; soil stabilization; subbases; subgrades

DOI: 10.14359/10332

Date: 5/1/1985

Abstract:
Methods are suggested for material selection, moisture control, and compaction or treatment of soils and materials to assure volume stability and uniform support for concrete pavements. Various environments are considered and appropriate methods of subgrade preparation are outlined. Subbase functions are defined and adaptability of types of subbases are discussed. Placement of materials to aid in subbase moisture control is emphasized in shoulder design. A section on recognition of causes of deficiencies in existing pavements is included to alert the engineer to the consequences of improper construction or adverse environment.