Behavior of Steel-to-Concrete Anchorages in High Moment Regions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Steel-to-Concrete Anchorages in High Moment Regions

Author(s): James D. Copley and Edwin G. Burdette

Publication: Journal Proceedings

Volume: 82

Issue: 2

Appears on pages(s): 180-187

Keywords: anchorage (structural); anchor bolts; concrete slabs; cracking (frac-turing); cyclic loads, moments; performance; pullout tests.

DOI: 10.14359/10326

Date: 3/1/1985

Abstract:
Tests were conducted to determine the relationship between curvature in a reinforced concrete slab and the behavior under cyfic loading of steel anchors embedded in the slab. Test results showed that the pullout deflection of the grouted bolts and self-drillers varied almost directly with slab curvature. The behavior of the wedge anchors was less well-defined because with each succeeding test performed on a set of wedge bolts the anchors siipped.further down the conical head of the bolt, producing increased resistance to pullout. Further re-search is needed to define better the relationship between anchor performance and level of applied moment.