334.2R-91: Reinforced Concrete Cooling Tower Shells -Practice and Commentary

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 334.2R-91: Reinforced Concrete Cooling Tower Shells -Practice and Commentary

Author(s): ACI Committee 334

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 9

Keywords: bending; buckling; columns (supports); concrete construction; cooling towers; earthquake resistant structures; earthquakes; loads (forces); membrane theory (shells); reinforced concrete: reinforcing steels; shells (structural forms); splicing; stability.

DOI:

Date: 1/1/1991

Abstract:
This document is an updated report on the design and construction of reinforced concrete cooling tower shells. In general, this report is addressed to towers 300 ft (90 m) or greater in height having a geometric form similar to or that of a hyperboloid of revolution. The specific intent is to provide the design profession with guidelines reflecting the present state of the art, as interpreted by the committee.