Title: 311.4R-00: Guide for Concrete Inspection

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 12

Keywords: concretes; construction; quality assurance; quality control; test.

DOI:

Date: 3/17/2000

Abstract:

Note: A newer version of this document exists. This document was replaced by 311.4R-05.

This guide discusses the need for inspection of concrete construction and other related activities, the types of inspection activities involved, and the responsibilities of various individuals and organizations involved in these activities. Field-testing activities are considered to be part of the inspection program. The guide presents recommended plans for the various types of inspection activities and means of implementing the program. Recommended minimum levels of inspection for various purposes and various types of projects are given.