Shear Strength of Reinforced High-Strength Concrete Deep Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Reinforced High-Strength Concrete Deep Beams

Author(s): Jung-Keun Oh and Sung-Woo Shin

Publication: Structural Journal

Volume: 98

Issue: 2

Appears on pages(s): 164-173

Keywords: beam; high-strength concrete; shear strength; span

DOI: 10.14359/10184

Date: 3/1/2001

Abstract:
Fifty-three reinforced concrete deep beams with compressive strengths in the range of 23 MPa £ fc¢ £ 74 MPa (3335 psi £ fc¢ £ 10,730 psi) were tested to determine their diagonal cracking and ultimate shear capacities symmetrically under two-point loading. The effective span-depth ratio le/d was varied from 3.0 to 5.0, and the shear span-effective depth ratio a/d from 0.5 to 2.0. All the beams were singly reinforced with ratio rt of 0.0129, 0.0156 and ratio of rv from 0 to 0.0034, and rh from 0 to 0.0094, respectively. The ultimate shear failure mode of deep beams was governed by a/d regardless of concrete strength. At a lower a/d, deep beams with high-strength concrete failed abruptly without any caution, which could be seen in deep beams with normal-strength concrete. Test results indicate that the ultimate shear strength of deep beams was determined predominantly by a/d. For all tested beams, ACI Code Eq. (11-29) and (11-30) are conservative and underestimate the effect of concrete compressive strength fc¢ and that of longitudinal steel reinforcement rt in deep beams using high-strength concrete. Addition of horizontal shear reinforcement does not improve the ultimate shear strength with decreasing a/d in deep beams with high-strength concrete


ALSO AVAILABLE IN:

Electronic Structural Journal