Deck Segmentation and Yard Organization for Launched Bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Deck Segmentation and Yard Organization for Launched Bridges

Author(s): Marco Rosignoli

Publication: Concrete International

Volume: 23

Issue: 2

Appears on pages(s): 64-73

Keywords:

DOI:

Date: 2/1/2001

Abstract:
Incremental bridge launching is a competitive construction method in a wide range of spans and bridge dimensions. Its competitiveness also derives from the repetitiveness of operations, which can be further enhanced by optimizing the deck segmentation according to the industrialization possibilities of the site and the criteria illustrated in the article. Particular cases such as precast segmental incremental launching and superstructures launched onto arches are also discussed.