Proposal for Standard Test of Modulus of Rupture of Concrete with Its Size Dependence

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposal for Standard Test of Modulus of Rupture of Concrete with Its Size Dependence

Author(s): Zdenlk P. Bauant and Drahomir Novak

Publication: Materials Journal

Volume: 98

Issue: 1

Appears on pages(s): 79-87

Keywords: concrete; fracture; modulus of rupture; stress

DOI: 10.14359/10164

Date: 1/1/2001

Abstract:
Recently accumulated test data on the modulus of rupture, as well as analytical studies and numerical simulations, clearly indicate that the flexural strength of concrete, called the modulus of rupture, significantly decreases as the beam size increases. This paper proposes a method to incorporate this size effect into the existing test standards, and focuses particularly on ASTM Standards C 78-94 and C 293-94. The proposed method is based on a recently established size effect formula that describes both the deterministic-energetic size effect caused by stress redistribution within the cross section due to finite size of the boundary layer of cracking at the tensile face of beam, and the classical Weibull-type statistical size effect due to the randomness of the local strength of material. Two alternatives of the test procedure are formulated. In the first alternative, beams of only one size are tested (as is recommended in the current standard), and the size effect on the mean modulus of rupture is approximately predicted on the basis of the average of existing information for all concretes. In the second alternative, beams of two sufficiently different sizes are tested. The latter is more tedious but gives a much better prediction of size effect for the concrete at hand; it allows for the estimation of size effect on not only the mean but also the coefficient of variation of the modulus of rupture (particularly, its decrease with increasing size). Numerical examples demonstrate the feasibility of the proposed approach.


ALSO AVAILABLE IN:

Electronic Materials Journal