Seismic Performance Evaluation of Cast-in-Steel-Shell (CISS) Piles

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Performance Evaluation of Cast-in-Steel-Shell (CISS) Piles

Author(s): Pedro Franco Silva and Frieder Seible

Publication: Structural Journal

Volume: 98

Issue: 1

Appears on pages(s): 36-49

Keywords: foundation; pile; strain

DOI: 10.14359/10145

Date: 1/1/2001

Abstract:
This paper describes experimental and analytical models developed at the University of California San Diego (UCSD) to evaluate the seismic response of cast-in-steel-shell (CISS) piles. Two CISS pile test units with different connection types to the pile cap were tested under varying axial and lateral loads. Test results showed that the embedment length of the steel shells into the pile cap, axial load variations, and the connection type influenced the lateral response of CISS piles. Observations recorded during testing were correlated with analytical predictions to characterize the load deformation response, predict damage levels and establish performance limit states for CISS piles under seismic loading.