Structural Design of Post-Tensioned Floors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Structural Design of Post-Tensioned Floors

Author(s): Bijan O Aalami, Gail S Kelley

Publication: Concrete International

Volume: 23

Issue: 1

Appears on pages(s): 31-36

Keywords:

DOI:

Date: 1/1/2001

Abstract:
This article presents the state-of-the-art in the design and application of post-tensioning in building construction. It summarizes the features of post-tensioning that have led to its wide acceptance in the United States and describes the principal design considerations. The basic concepts of post-tensioned construction are discussed and both common construction geometries and limiting design factors are introduced.