Strength Development of Blended Blast Furnace Slag Cement Mortars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength Development of Blended Blast Furnace Slag Cement Mortars

Author(s): C. L. Hwang and C. Y. Lin

Publication: Symposium Paper

Volume: 91

Issue:

Appears on pages(s): 1323-1340

Keywords: alkalies; batching; blast furnace slag; bleeding (concrete); cooling; diffusion; fineness; flash set; grinding (comminution); mixing; mortars (material); porosity; strength.

DOI: 10.14359/10124

Date: 2/1/1986

Abstract:
Blast-furnace slags cooled at different rates were used to study the effect of fineness, mixing method and content of slag on the strength development of blended-slag mortar. Test results indicated that the strength development of air-cooled slag was better than expected, even though it was less effective than that of water quenched. When the intergrinding method was compared with the separate batching method, the latter needs a longer mixing time to reach a comparable quality. The slump and bleeding were reduced as the amount of slag increased at low water to cementitious mix ratio. Alkali activated the reaction of slag. However, excessive alkali might cause flash setting of the fresh mortar. The diffusion process seemed to govern the cementitious reaction of slag and which, in turn, tended to retard the hydra-tion of cement. Therefore, the optimum slag content depended upon the age of cement mortar.