Effects of Different Fly Ashes and Silica Fume on Selected Properties of an Expansive Grout

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Different Fly Ashes and Silica Fume on Selected Properties of an Expansive Grout

Author(s): L. D. Wakeley and A. D. Buck

Publication: Symposium Paper

Volume: 91

Issue:

Appears on pages(s): 1261-1278

Keywords: compressive strength; expanding agents; expansion; fly ash; grouts; microstructure; permeability; silica; x-ray diffraction.

DOI: 10.14359/10121

Date: 2/1/1986

Abstract:
An expansive grout, based on Class H cement, an expan- sive admixture consisting essentially of plaster of paris (calcium sulfate hemihydrate), and a Class C fly ash, was proportioned for use underground. Specimens of this grout, and of five modified versions of it, were tested to determine the effects of using two ther fly ashes, with or without silica fume, on compressive strength, volume change, phase composition, and microstructure. Properties were monitored to 960-days age. Up to 365-days age, specimens of the mixture modified with Class F fly ash had lower compressive strengths and generally more expansion than did those of the original composition. At ages of 90 days and greater, the same was true of samples prepared with a second Class C fly ash. Substitution of silica fume for 5 or 10 percent of the cement gave higher early strength, but the combination of the second Class C fly ash and 10 percent silica fume gave the lowest strengths at ages of 90 days and greater. Despite the substitutions, properties were markedly similar, compressive strength from all modifications exceeded 90 MPa at 365 days, and phase composition and microstructures became more similar with time.