Effect of Condensed Silica Fume on the Strength Development of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Condensed Silica Fume on the Strength Development of Concrete

Author(s): Malvin Sandvik and Odd E. Gjorv

Publication: Symposium Paper

Volume: 91

Issue:

Appears on pages(s): 893-902

Keywords: age-strength relation; cement content; compressive strength; concretes; silica.

DOI: 10.14359/10102

Date: 2/1/1986

Abstract:
The effect of condensed silica fume on the strength deve-lopment in concrete was studied by replacement of 0, 5,10, and 20% cement by silica fume. No admixtures was used. For all the mixes,about the same strength was obtained up to 7 days. From then on,the mixes with silica fume produced an increased strength development compared to that of pure cement. At a partial replacement of cement by 20%, the compressive strength at 28 and 90 days was increased by 43 and 55%, respectively, with respect to the strength at 7 days.