Production and Utilization of Fly Ash in Italy

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Production and Utilization of Fly Ash in Italy

Author(s): G. L. Valenti, R. Cioffi, and R. Sersale

Publication: Symposium Paper

Volume: 91

Issue:

Appears on pages(s): 741-762

Keywords: Blaine method; calcium oxides; cements; chemical analysis; fly ash; lime; mechanical properties; mortars (material); particle size distribution; pozzolans; strength.

DOI: 10.14359/10095

Date: 2/1/1986

Abstract:
The fly ashes produced in Italy generally show good pozzolanic behaviour. Tests made on lime and cement mortars have shown that 4 of the 5 ashes give comparable or even superior performance to that of a natural pozzolan usually employed in the production of portland pozzolan cements. The chemical characteristics were: Si02 42.7-50.2%; Si02+A1203 66.5-77.2%; Si02+A1203+Fe203 75.8-83.5%; loss on ignition 3.9-12.9% and CaO 1.8-9.3%. The calcium oxide content is the parameter that greatly influences the technical behaviour. Glass content ranging from 63 to 75% does not have a dominant influence on mechanical strength. The particle size distribution, rather than the fraction <45pm determines the mechanical characteristics.