Behavior of a New Steel-Concrete Hybrid Frame System

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of a New Steel-Concrete Hybrid Frame System

Author(s): R. S. Aboutaha

Publication: Symposium Paper

Volume: 196

Issue:

Appears on pages(s): 175-188

Keywords: confinement;ductility; headed bars; plastic hinge; reinforced concrete; seismic resistance; shear resistance; steel tube

DOI: 10.14359/10010

Date: 10/1/2000

Abstract:
the reinforcing bars and the surrounding concrete within the beam column joint. This paper introduces a new innovative steel-concrete composite frame system with controlled plastic mechanism. This frame system consists of steel tubed reinforced concrete (STRC) columns, and ordinary reinforced concrete beams with relocated plastic hinges. Beam plastic hinges are relocated by the use of straight headed bars. The STRC column is an ordinary reinforced concrete column but, transversely reinforced with light ordinary ties and a thin steel tube. Compared to concrete filled tube column (CFT), the steel tube of STRC column transfers no axial load, provides better confinement, and consequently, increases column ductility. In this paper, experimental investigation of two full scale STRC columns and two beams with and without headed bars are presented. Test results suggest that STRC columns and beams with relocated plastic hinge regions could offer a more ductile structural frame system for medium and high rise buildings in zones of high seismicity.