Title: Should I Use ACI 318 or LRFD for Designing Composite Columns?

Author(s): R. W. Furlong

Publication: Symposium Paper

Volume: 196

Issue:

Appears on pages(s): 125-140

Keywords: columns; composite; design; load factors

DOI: 10.14359/10001

Date: 10/1/2000

Abstract:
Steel-concrete composite columns may be designed either by requirements of the American Concrete Institute Building Code AC1 3 18-99 or by the American Institute of Steel Construction Specifications for Load and Resistance Factor Design, 2d Edition (1995). Each design standard is described for application to a concrete filled steel tube and to a concrete encased structural shape as each is designed for the same dimensional and service load conditions. These standard type column sections are used for the comparison, as the LRFD specification can be used directly only for such standard sections. The design exercise demonstrates that a) the LRFD specification requires fewer computational steps and is therefore easier to apply, b) the ACI rules tend to exaggerate the influence of slenderness, and c) different but very similar results were obtained for the two methods applied to the same design problem.