Title: Fire-Testing Epoxies

Author(s): Joseph M. Plecnik, John Plecnik, Victor parra, Ahmad Diba

Publication: Concrete International

Volume: 8

Issue: 4

Appears on pages(s): 29-33

Keywords:

DOI:

Date: 4/1/1986

Abstract:
With the increasing use of epoxy adhesives in the repair and strengthening of concrete structures, the risk for elevated temperature or fire exposure on epoxy-repaired concrete elements is also increased. The authors have investigated the effects of fire exposure on epoxy-repaired concrete beams, determined the effectiveness of a plaster coating applied to epoxy-repaired beams, and evaluated deflections and strength.