Proposed Revisions to ACI Standard: Recommended Practice for Selecting Proportions for Normal and Heavyweight Concrete (ACI 211 .l-77)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Revisions to ACI Standard: Recommended Practice for Selecting Proportions for Normal and Heavyweight Concrete (ACI 211 .l-77)

Author(s): ACI Committee 211

Publication: Concrete International

Volume: 2

Issue: 12

Appears on pages(s): 67-70

Keywords: absorption; aggregates; air-entrained con-cretes; air entrainment; cement content; coarse ag-gregates; concrete durability; concretes; consistency; durability; exposure; fine aggregates;

DOI:

Date: 12/1/1980

Abstract:
Describes, with examples, two methods for selecting and adjusting proportions for normal weight concrete. One method is based on an estimated weight of the concrete per unit volume; the other is based on calculations of the absolute volume occupied by the concrete ingredients. The procedures take into con-sideration the requirements for placeability, consistency, strength, and durability. Example calculations are shown for both methods, including adjust-ments based on the characteristics of the first trial batch. The proportioning of heavyweight concrete for such purposes as radiation shielding and bridge counterweight structures is described in an appendix. This appendix uses the absolute volume method which is generally accepted and is more convenient for heavyweight concrete.




  