Title: Studies of Autogenous Volume Change in Concrete for Dworshak Dam

Author(s): Ivan E. Houk, Jr., Orville E. Borge, and Donald L. Houghton

Publication: Journal Proceedings

Volume: 66

Issue: 7

Appears on pages(s): 560-568

Keywords: aggregate gradation; cement content;compressive strength; concretes; cooling; fineness; fly ash; mass concrete; mix proportioning; portland cements; pozzolans; pumice; shales; shrinkage; slags; strains; stresses; volume change.

DOI: 10.14359/7381

Date: 7/1/1969

Abstract:
The autogenous volume change was measured in mass concrete mixtures having cementing materials, portland cement, and pozzolan, ranging from 222 to 302 lb per cu yd ( I32 to 179 kg/m3 l Some concrete contained pozzolans replacing 30 percent of the portland cement by absolute volume and others contained no pozzolan. One mixture contained a 50 percent pozzolan replacement. Seven pozzolans from a wide range of sources were used. Observation periods have extended to 3 years. This investigation was performed in connection with the U.S. Army Corps of Engineers’ design of Dworshak Dam, North Fork Clearwater River near Orofino, Idaho.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer