Confinement Reinforcement of Cyclically Loaded Normal-Strength Concrete Tied Columns under High Axial Loads (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Confinement Reinforcement of Cyclically Loaded Normal-Strength Concrete Tied Columns under High Axial Loads (Prepublished)

Author(s): Wen-Cheng Shen and Shyh-Jiann Hwang

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: column; confining reinforcement; crosstie configuration; high axial load; ultimate drift ratio

DOI: 10.14359/51749406

Date: 12/18/2025

Abstract:

In high-rise buildings, lower-story columns must withstand significant seismic shear forces while maintaining sufficient deformation capacity. This capacity is provided through effective confinement using transverse reinforcement. The ACI 318-25 building code specifies that confining reinforcement should be proportional to the applied axial load when the axial load exceeds 0.3Agf'c and requires all longitudinal bars to be laterally supported with seismic hooks. However, the implementation of seismic hooks at both ends of crossties brings challenges for on-site reinforcement assembly.

This study experimentally investigates full-scale RC column specimens subjected to quasi-static cyclic loading while under a constant high axial load. The objectives are to validate the ACI 318-25 confinement requirements and to evaluate the feasibility of relaxing seismic hook requirements. The results confirm that columns designed in accordance with the ACI 318-25 building code satisfy the required 3% deformation capacity. Furthermore, satisfactory seismic performance can be achieved with crossties incorporating alternating 135-degree and 90-degree hooks, although at the expense of increased confining reinforcement.