A Mathematical Framework for Computing Polar Moments of Inertia for Use with the Traditional ‘ACI Commentary Jc Method’ (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Mathematical Framework for Computing Polar Moments of Inertia for Use with the Traditional ‘ACI Commentary Jc Method’ (Prepublished)

Author(s): Hugo Esquivel and Guang Lin

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: ACI 318-25; Jc method; (centroidal) polar moment of inertia; slab-column connection; structural design; two-way shear action

DOI: 10.14359/51749378

Date: 12/8/2025

Abstract:
This article presents a robust mathematical framework for computing centroidal polar moments of inertia in a standardized manner, applicable to both regular- and irregular-shaped sections, for use with the traditional ‘ACI Commentary Jc Method.’ The article also showcases with mathematical rigor why, for over 60 years, the standard (traditional) expressions used to compute polar moments of inertia for planar sections embedded in three-dimensional space have been incorrectly derived, and explores the implications of not adopting the correct expressions in design. The mathematical framework for computing polar moments of inertia is developed using advanced calculus, and primitive sections are integrated into the formulation to derive with ease the necessary expressions for the most common sections used in design, namely: rectangular, circular, C-shaped, L-shaped, and regular polygon-shaped sections. Finally, a numerical example is provided to demonstrate the practical implementation of the proposed mathematical framework.