Title: Model for corrosion initiation and propagation based on the resistivity

Author(s): Carmen Andrade

Publication: Symposium Paper

Volume: 366

Issue:

Appears on pages(s): 156-169

Keywords: model, service-lie, corrosion, initiation, propagation, resistivity

DOI: 10.14359/51749240

Date: 10/1/2025

Abstract:
Concrete is an efficient material in terms of mechanical strength and functionality, but whose durability is one of present challenges that need particular attention to preserve the reinforcement absent of corrosion during the nominal service life. Present trends on modelling by performance make more complex the quality control testing and lengthens the characterization of new low carbon cement concretes. In present work is presented concrete resistivity as the single parameter able to characterize both corrosion periods through the corresponding mathematical expressions. Resistivity is a non-destructive test which could qualify concrete from its early ages. Based in the relation between diffusivity-corrosion current and resistivity, an integral model based in the resistivity measured at short term in the same specimens than mechanical strength (cured humid), is described. It is also analysed the analogies between the diffusivity and corrosion current and the influence of climate in the resistivity for future challenge of predicting the impact of climatic change.




  