Title:
Concrete Q&A: GFRP Misconceptions—Part 1
Author(s):
Publication:
Concrete International
Volume:
47
Issue:
10
Appears on pages(s):
93-96
Keywords:
reinforcing, bar, code, test
DOI:
Date:
10/1/2025
Abstract:
This is the first in the series of Q&A articles clarifying some common questions and misconceptions about glass fiber-reinforced polymer (GFRP) reinforcing bars. Discussed topics include codes and standards for GFRP bars, requirements and testing, degradation mechanisms, construction, bending, and tariffs and supply.