Constructability in Cold Weather Conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Constructability in Cold Weather Conditions

Author(s): Keila Heitmeyer

Publication: Concrete International

Volume: 47

Issue: 10

Appears on pages(s): 62-63

Keywords: concrete, project, guide, session

DOI:

Date: 10/1/2025

Abstract:
Cold weather conditions pose constructability challenges when placing and testing to ensure a sound product. The key to successfully executing field work in cold weather conditions is to plan diligently while considering recommendations from ACI 306R-16, “Guide to Cold Weather Concreting.”




  