Residual Bond of GFRP Bars Embedded in UHPC at Elevated Temperatures (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Residual Bond of GFRP Bars Embedded in UHPC at Elevated Temperatures (Prepublished)

Author(s): Yail J. Kim and Ali Alatify

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: fiber-reinforced polymer (FRP); interface; reinforcement; residual bond; thermal load; ultra-high performance concrete (UHPC)

DOI: 10.14359/51749172

Date: 9/11/2025

Abstract:
This paper presents an experimental study on the residual bond of glass fiber-reinforced polymer (GFRP) rebars embedded in ultra-high-performance concrete (UHPC) subjected to elevated temperatures, including a comparison with ordinary concrete. Based on the range of thermal loading from 25°C (77°F) to 300o°C (572o°F), material and push-out tests are conducted to examine the temperature-dependent properties of the constituents and the behavior of the interface. Also performed are chemical and radiometric analyses. The average specific heat and thermal conductivity of UHPC are 12.1% and 6.1% higher than those of ordinary concrete, respectively. The temperature-induced reduction of density in these mixtures ranges between 5.4% and 6.2% at 300o°C (572o°F). Thermal damage to GFRP, in the context of microcracking, is observed after exposure to 150°C (302°F). Fourier transform infrared spectroscopy reveals prominent wavenumbers at 668 cm-1 (263 in.-1) and 2,360 cm-1 (929 in.-1), related to the bond between the fibers and resin in the rebars, while spectroradiometry characterizes the thermal degradation of GFRP through diminished reflectivity in conjunction with the peak wavelength positions of 584 nm (2,299×10-8 in.) and 1,871 nm (7,366×10-8 in.). The linearly ascending bond-slip response of the interface alters after reaching the maximum shear stresses, leading to gradual and abrupt declines for the ordinary concrete and UHPC, respectively. The failure mode of the ordinary concrete interface is temperature-sensitive; however, spalling in the bonded region is consistently noticed in the UHPC interface. The fracture energy of the interface with UHPC exceeds that of the interface with the ordinary concrete beyond 150o°C (302o°F). Design recommendations are provided for estimating reductions in the residual bond of the GFRP system exposed to elevated temperatures.