Ultimate Flexure Strength Evaluation of Reinforced Concrete Beams Retrofitted with Carbon Fiber-Reinforced Polymer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ultimate Flexure Strength Evaluation of Reinforced Concrete Beams Retrofitted with Carbon Fiber-Reinforced Polymer

Author(s): Jorge L. Bazan and Victor I. Fernandez-Davila

Publication: Structural Journal

Volume: 123

Issue: 1

Appears on pages(s): 201-218

Keywords: carbon fiber-reinforced polymer (CFRP) flexural strengthening; probable moment strength; reinforced concrete (RC) beam; shear capacity design; ultimate flexure strength

DOI: 10.14359/51749171

Date: 1/1/2026

Abstract:
This study investigates the ultimate flexural strength (UFS) of reinforced concrete beams strengthened with carbon fiber-reinforced polymer (CFRP) (RCB-SCFRP), focusing on the identification and quantification of flexural overstrength concerning the nominal flexural strength (NFS) as defined by ACI 440.2R. A total of 106 full-scale specimens tested were carefully selected from previous research, varying in concrete strength, reinforcement configurations, and CFRP materials from multiple manufacturers. Results show that ACI 440.2R provisions accurately and conservatively estimate the flexural capacity of CFRP-strengthened beams. Including CFRP transverse reinforcement (TR) resulted in a slight increase in UFS. The type of strengthening, whether preloaded and repaired or strengthened, had little effect on the UFS/NFS ratio. Steel reinforcement ratio (SRR) significantly influenced overstrength, with higher UFS/NFS ratios observed between 0.70% and 1.00% SRR. CFRP axial rigidity (Kf ρf) notably affected overstrength, with optimal performance between 0.10 and 0.50 GPa·mm. Deflection ductility was mainly affected by the rigidity of CFRP, with a 13% increase noted due to CFRP TR. A log-normal model was developed to estimate UFS for RCB-SCFRP beams based on experimental data and ACI 440.2R guidelines.

Related References:

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 624 pp.

ACI Committee 440, 2017, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-17),” American Concrete Institute, Farmington Hills, MI, 112 pp.

Al-Salloum, Y. A.; Almusallam, T. H.; Alsayed, S. H.; and Siddiqui, N. A., 2011, “Seismic Behavior of As-Built, ACI-Complying, and CFRP-Repaired Exterior RC Beam-Column Joints,” Journal of Composites for Construction, ASCE, V. 15, No. 4, pp. 522-534. doi: 10.1061/(ASCE)CC.1943-5614.0000186

Al-zu’bi, H.; Abdel-Jaber, M.; and Katkhuda, H., 2022, “Flexural Strengthening of Reinforced Concrete Beams with Variable Compressive Strength Using Near-Surface Mounted Carbon-Fiber-Reinforced Polymer Strips [NSM-CFRP],” Fibers, V. 10, No. 10, p. 86. doi: 10.3390/fib10100086

Alabdulhady, M. Y.; Ojaimi, M. F.; and Chkheiwer, A. H., 2022, “The Efficiency of CFRP Strengthening and Repair System on the Flexural Behavior of RC Beams Constructed with Different Concrete Compressive Strength,” Results in Engineering, V. 16, p. 100763. doi: 10.1016/j.rineng.2022.100763

Aram, M. R.; Czaderski, C.; and Motavalli, M., 2008, “Debonding Failure Modes of Flexural FRP-Strengthened RC Beams,” Composites Part B: Engineering, V. 39, No. 5, pp. 826-841. doi: 10.1016/j.compositesb.2007.10.006

Askar, M. K.; Hassan, A. F.; and Al-Kamaki, Y. S. S., 2022, “Flexural and Shear Strengthening of Reinforced Concrete Beams Using FRP Composites: A State of the Art,” Case Studies in Construction Materials, V. 17, p. e01189. doi: 10.1016/j.cscm.2022.e01189

Assad, M.; Hawileh, R. A.; and Abdalla, J. A., 2024, “Flexural Strengthening of Reinforced Concrete Beams with CFRP Laminates and Spike Anchors,” Composites Part C: Open Access, V. 13, p. 100443. doi: 10.1016/j.jcomc.2024.100443

Attari, N.; Amziane, S.; and Chemrouk, M., 2012, “Flexural Strengthening of Concrete Beams Using CFRP, GFRP and Hybrid FRP Sheets,” Construction and Building Materials, V. 37, pp. 746-757. doi: 10.1016/j.conbuildmat.2012.07.052

Baggio, D.; Soudki, K.; and Noël, M., 2014, “Strengthening of Shear Critical RC Beams with Various FRP Systems,” Construction and Building Materials, V. 66, pp. 634-644. doi: 10.1016/j.conbuildmat.2014.05.097

Bazán, J.; Samaniego, J.; and Fernández-Dávila, V., 2020, “Use of FRP Anchorages in Reinforced Concrete Beams Externally Strengthened with CFRP Bands Subjected to Cyclic Loads,” Revista Ingeniería, V. 30, No. 2, pp. 77-94. doi: 10.15517/ri.v30i2.39806

Bazan, J. L., and Fernandez-Davila, V. I., 2020, “Evaluation of the Experimental Curvature Ductility of RC Beams Externally Strengthened with CFRP Bands,” Structures, V. 26, pp. 1010-1020. doi: 10.1016/j.istruc.2020.04.030

Belarbi, A., and Acun, B., 2013, “FRP Systems in Shear Strengthening of Reinforced Concrete Structures,” Procedia Engineering, V. 57, pp. 2-8. doi: 10.1016/j.proeng.2013.04.004

Bouzid, H.; Rabia, B.; and Daouadji, T. H., 2023, “Ultimate Behavior of RC Beams Strengthened in Flexure Using FRP Material,” Engineering Structures, V. 289, May, p. 116300. doi: 10.1016/j.engstruct.2023.116300

Ceroni, F., 2010, “Experimental Performances of RC Beams Strengthened with FRP Materials,” Construction and Building Materials, V. 24, No. 9, pp. 1547-1559. doi: 10.1016/j.conbuildmat.2010.03.008

Choobbor, S. S.; Hawileh, R. A.; Abu-Obeidah, A.; and Abdalla, J. A., 2019, “Performance of Hybrid Carbon and Basalt FRP Sheets in Strengthening Concrete Beams in Flexure,” Composite Structures, V. 227, p. 111337. doi: 10.1016/j.compstruct.2019.111337

del Rey Castillo, E., and Kanitkar, R., 2021, “Effect of FRP Spike Anchor Installation Quality and Concrete Repair on the Seismic Behavior of FRP-Strengthened RC Columns,” Journal of Composites for Construction, ASCE, V. 25, No. 1, p. 04020085. doi: 10.1061/(ASCE)CC.1943-5614.0001095

Dong, Y., and Ansari, F., 2002, “Failure Characteristics of Reinforced Concrete Beams Repaired with CFRP Composites,” 14 pp.

Fernandez-Davila, V. I.; Gutierrez, M. M. M.; Samaniego, J. D.; Bazan, J. L.; and Santa-Cruz, S., 2022, “Flexural Behavior of Reinforced Concrete Beams Strengthened with Composite Carbon Fiber-Reinforced Polymer System,” ACI Structural Journal, V. 119, No. 3, May, pp. 221-231. doi: 10.14359/51734346

Fu, B.; Chen, G. M.; and Teng, J. G., 2017, “Mitigation of Intermediate Crack Debonding in FRP-Plated RC Beams Using FRP U-Jackets,” Composite Structures, V. 176, pp. 883-897. doi: 10.1016/j.compstruct.2017.05.049

GangaRao, H. V. S., and Vijay, P. V., 1998, “Bending Behavior of Concrete Beams Wrapped with Carbon Fabric,” Journal of Structural Engineering, ASCE, V. 124, No. 1, pp. 3-10. doi: 10.1061/(ASCE)0733-9445(1998)124:1(3)

Hamrat, M.; Bouziadi, F.; Boulekbache, B.; Daouadji, T. H.; Chergui, S.; Labed, A.; and Amziane, S., 2020, “Experimental and Numerical Investigation on the Deflection Behavior of Pre-Cracked and Repaired Reinforced Concrete Beams with Fiber-Reinforced Polymer,” Construction and Building Materials, V. 249, p. 118745. doi: 10.1016/j.conbuildmat.2020.118745

Hollings, J. P., 1969, “Reinforced Concrete Seismic Design,” Bulletin of the New Zealand Society for Earthquake Engineering, V. 2, No. 3, pp. 217-250. doi: 10.5459/bnzsee.2.3.217-250

Hosny, A.; Shaheen, H.; Abdelrahman, A.; and Elafandy, T., 2006, “Performance of Reinforced Concrete Beams Strengthened by Hybrid FRP Laminates,” Cement and Concrete Composites, V. 28, No. 10, pp. 906-913. doi: 10.1016/j.cemconcomp.2006.07.016

Kachlakev, D., 2002, “Horsetail Creek Bridge: Design Method Calibration and Experimental Results of Structural Strengthening with CFRP and GFRP Laminate,” Advances in Structural Engineering, V. 5, No. 2, pp. 87-98. doi: 10.1260/1369433021502588

Ke, Y.; Zhang, S.; Smith, S.; and Yu, T., 2023, “Novel Embedded FRP Anchor for RC Beams Strengthened in Flexure with NSM FRP Bars: Concept and Behavior,” Journal of Composites for Construction, ASCE, V. 27, No. 1, p. 04022093. doi: 10.1061/(ASCE)CC.1943-5614.0001279

Kim, G.; Sim, J.; and Oh, H., 2008, “Shear Strength of Strengthened RC Beams with FRPs in Shear,” Construction and Building Materials, V. 22, No. 6, pp. 1261-1270. doi: 10.1016/j.conbuildmat.2007.01.021

Kim, N.; Kim, Y.; and Sun Kim, H., 2013, “Experimental Study for Evaluating Structural Behavior of RC Beams Strengthened by Different Width of FRP Layers,” IACSIT International Journal of Engineering and Technology, V. 5, No. 6, pp. 662-665. doi: 10.7763/IJET.2013.V5.637

Lin, Y.; Wei, Y.; Gong, Z.; Xu, W.; and Zhao, K., 2024, “Flexural Behavior of an RC Beam Externally Strengthened with a Steel- and CFRP-Based Method,” Applied Sciences, V. 14, No. 20, p. 9281. doi: 10.3390/app14209281

Mastali, M., and Dalvand, A., 2016, “The Impact Resistance and Mechanical Properties of Self-Compacting Concrete Reinforced with Recycled CFRP Pieces,” Composites Part B: Engineering, V. 92, pp. 360-376. doi: 10.1016/j.compositesb.2016.01.046

Mostofinejad, D., and Akhlaghi, A., 2017, “Flexural Strengthening of Reinforced Concrete Beam- Column Joints Using Innovative Anchorage System,” ACI Structural Journal, V. 114, No. 6, Nov.-Dec., pp. 1603-1614. doi: 10.14359/51700953

Mugahed Amran, Y. H.; Alyousef, R.; Rashid, R. S. M.; Alabduljabbar, H.; and Hung, C. C., 2018, “Properties and Applications of FRP in Strengthening RC Structures: A Review,” Structures, V. 16, pp. 208-238. doi: 10.1016/j.istruc.2018.09.008

Namboorimadathil, S. M.; Tumialan, J. G.; and Nanni, A., 2002, “Behavior of RC T-Beams Strengthened in the Negative Moment Region with CFRP Laminates,” 9 pp.

Naser, M. Z.; Hawileh, R. A.; and Abdalla, J. A., 2019, “Fiber-Reinforced Polymer Composites in Strengthening Reinforced Concrete Structures: A Critical Review,” Engineering Structures, V. 198, p. 109542. doi: 10.1016/j.engstruct.2019.109542

Nawaz, W.; Elchalakani, M.; Karrech, A.; Yehia, S.; Yang, B.; and Youssf, O., 2022, “Flexural Behavior of All Lightweight Reinforced Concrete Beams Externally Strengthened with CFRP Sheets,” Construction and Building Materials, V. 327, p. 126966. doi: 10.1016/j.conbuildmat.2022.126966

Nguyen, N. T.; Nguyen, T. K.; Du, D. H.; Nguyen, D. N.; and Kieu, T. S., 2023, “Nonlinear Finite Element Analysis of FRP-Strengthened Full-Size Reinforced Concrete Beams,” Innovative Infrastructure Solutions, V. 8, p. 139.

Okeil, A. M.; Bingol, Y.; and Alkhrdaji, T., 2007, “Analyzing Model Uncertainties for Concrete Beams Flexurally Strengthened with FRP Laminates,” Transportation Research Board 86th Annual Meeting, Washington, DC.

Park, R., and Paulay, T., 1991, Reinforced Concrete Structures, John Wiley & Sons, New York.

Proaño, R., 2011, “Comportamiento de Vigas de concreto armado reforzadas externamente con platinas de Fibras de Carbono,” master’s thesis, Universidad Nacional de Ingeniería, Lima, Peru.

Quattlebaum, J. B.; Harries, K. A.; and Petrou, M. F., 2005, “Comparison of Three Flexural Retrofit Systems under Monotonic and Fatigue Loads,” Journal of Bridge Engineering, ASCE, V. 10, No. 6, pp. 731-740. doi: 10.1061/(ASCE)1084-0702(2005)10:67310.1061/(ASCE)1084-0702(2005)10:6

Restrepo, J. I., and Rodriguez, M. E., 2013, “On the Probable Moment Strength of Reinforced Concrete Columns,” ACI Structural Journal, V. 110, No. 4, July-Aug., pp. 681-690. doi: 10.14359/51685753

Spadea, G.; Swamy, R. N.; and Bencardino, F., 2001, “Strength and Ductility of RC Beams Repaired with Bonded CFRP Laminates,” Journal of Bridge Engineering, ASCE, V. 6, No. 5, pp. 349-355. doi: 10.1061/(ASCE)1084-0702(2001)6:53410.1061/(ASCE)1084-0702(2001)6:5

Toutanji, H.; Zhao, L.; and Zhang, Y., 2006, “Flexural Behavior of Reinforced Concrete Beams Externally Strengthened with CFRP Sheets Bonded with an Inorganic Matrix,” Engineering Structures, V. 28, No. 4, pp. 557-566. doi: 10.1016/j.engstruct.2005.09.011

Wattanapanich, C.; Imjai, T.; Garcia, R.; Rahim, N. L.; Abdullah, M. M. A. B.; Sandu, A. V.; Vizureanu, P.; Matasaru, P. D.; and Thomas, B. S., 2023, “Computer Simulations of End-Tapering Anchorages of EBR FRP-Strengthened Prestressed Concrete Slabs at Service Conditions,” Materials, V. 16, No. 2, p. 851. doi: 10.3390/ma1602085


ALSO AVAILABLE IN:

Electronic Structural Journal