Title:
Long-Term Impact Behavior of Basalt Fiber-Reinforced Polymer-Seawater Sea-Sand Concrete Beams Under Marine Environment
Author(s):
Deju Zhu, Guoxi Zeng, Weilin Zhong, Weijian Yi, and Shuaicheng Guo
Publication:
Structural Journal
Volume:
123
Issue:
2
Appears on pages(s):
129-144
Keywords:
basalt fiber-reinforced polymer (BFRP) bar; drop-weight impact; impact behavior; seawater sea-sand concrete (SSC) beam
DOI:
10.14359/51749167
Date:
3/1/2026
Abstract:
The influence of alkaline aging on basalt fiber-reinforced polymer (BFRP) bar-reinforced concrete beams has not been thoroughly investigated, and the deterioration level can be further increased in seawater sea-sand concrete (SSC) due to increased alkalinity. This study aims to unveil the coupled influence mechanism of accelerated seawater aging and impact loading on the impact resilience of BFRP-SSC beams. The influence of concrete strength, reinforcement ratio, falling weight height, and accelerated aging in seawater on the impact resistance of BFRP-SSC beams is examined. The results indicate that enhancing concrete strength can increase the peak impact force more significantly than increasing the reinforcement ratio, due to the higher strain-rate sensitivity. The increased drop-weight energy can increase the peak impact force while reducing the residual bearing capacity. The accelerated aging in seawater can reduce the peak impact force and increase the maximum midspan displacement. Furthermore, the impact failure mode of the BFRP-SSC beam can be changed from concrete crushing to BFRP bar fracture due to the bar degradation. The peak impact forces of beam specimens soaked in seawater at room temperature and 55°C conditions were reduced by 13.8% and 15.5%, while the maximum midspan displacements were increased by 32.2% and 47.1%, respectively. This study can serve as a solid base for the impact design of FRP bar-reinforced seawater sea-sand concrete beams.
Related References:
1. Guo, M.; Hu, B.; Xing, F.; Zhou, X.; Sun, M.; Sui, L.; and Zhou, Y., “Characterization of the Mechanical Properties of Eco-Friendly Concrete Made with Untreated Sea Sand and Seawater Based on Statistical Analysis,” Construction and Building Materials, V. 234, Feb. 2020, Article No. 117339. doi: 10.1016/j.conbuildmat.2019.117339
2. Yan, F.; Lin, Z.; and Yang, M., “Bond Mechanism and Bond Strength of GFRP Bars to Concrete: A Review,” Composites Part B: Engineering, V. 98, Aug. 2016, pp. 56-69. doi: 10.1016/j.compositesb.2016.04.068
3. Sadraie, H.; Khaloo, A.; and Soltani, H., “Dynamic Performance of Concrete Slabs Reinforced with Steel and GFRP Bars Under Impact Loading,” Engineering Structures, V. 191, July 2019, pp. 62-81. doi: 10.1016/j.engstruct.2019.04.038
4. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.
5. Montanari, L.; Suraneni, P.; Tsui-Chang, M.; Khatibmasjedi, M.; Ebead, U.; Weiss, J.; and Nanni, A., “Hydration, Pore Solution, and Porosity of Cementitious Pastes Made with Seawater,” Journal of Materials in Civil Engineering, ASCE, V. 31, No. 8, Aug. 2019, p. 04019154. doi: 10.1061/(ASCE)MT.1943-5533.0002818
6. Yi, Y.; Zhu, D.; Guo, S.; Li, S.; Feng, G.; Liu, Z.; Zhou, L.; and Shi, C., “Development of a Low-Alkalinity Seawater Sea Sand Concrete for Enhanced Compatibility with BFRP Bar in the Marine Environment,” Cement and Concrete Composites, V. 134, Nov. 2022, Article No. 104778. doi: 10.1016/j.cemconcomp.2022.104778
7. Yi, Y.; Zhu, D.; Rahman, M. Z.; Shuaicheng, G.; Li, S.; Liu, Z.; and Shi, C., “Tensile Properties Deterioration of BFRP Bars in Simulated Pore Solution and Real Seawater Sea Sand Concrete Environment with Varying Alkalinities,” Composites Part B: Engineering, V. 243, Aug. 2022, Article No. 110115. doi: 10.1016/j.compositesb.2022.110115
8. AASHTO, “AASHTO LRFD Bridge Design Guide Specifications for GFRP-Reinforced Concrete Bridge Decks and Traffic Railings,” first edition, American Association of State Highway and Transportation Officials, Washington, DC, 2009, 66 pp.
9. Zhu, D.; Zhong, W.; Xu, Z.; Liu, Z.; Guo, S.; and Li, A., “Impact Resistance of Seawater Sea-Sand Concrete Beams Reinforced with BFRP Bars,” Journal of Vibration and Shock, V. 42, No. 14, 2023, pp. 220-228.
10. Toutanji, H. A., and Saafi, M., “Flexural Behavior of Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars,” ACI Structural Journal, V. 97, No. 5, Sept.-Oct. 2000, pp. 712-719.
11. Fan, X., and Zhang, M., “Experimental Study on Flexural Behaviour of Inorganic Polymer Concrete Beams Reinforced with Basalt Rebar,” Composites Part B: Engineering, V. 93, May 2016, pp. 174-183. " target="_blank">doi: 10.1016/j.compositesb.2016.03.021
12. Dong, Z.; Sun, Y.; Zhu, H.; Wu, G.; and Shao, X., “Shear Behavior of Hybrid Seawater Sea-Sand Concrete Short Beams Reinforced with BFRP Reinforcements,” Engineering Structures, V. 252, Feb. 2022, Article No. 113615. doi: 10.1016/j.engstruct.2021.113615
13. Saleh, Z.; Sheikh, M. N.; Remennikov, A.; and Basu, A., “Damage Assessment of GFRP Bar Reinforced Ultra-High-Strength Concrete Beams Under Overloading Impact Conditions,” Engineering Structures, V. 213, June 2020, Article No. 110581. doi: 10.1016/j.engstruct.2020.110581
14. Goldston, M. W.; Remennikov, A.; Saleh, Z.; and Sheikh, M. N., “Experimental Investigations on the Behavior of GFRP Bar Reinforced HSC and UHSC Beams Under Static and Impact Loading,” Structures, V. 22, Dec. 2019, pp. 109-123. doi: 10.1016/j.istruc.2019.08.002
15. Goldston, M.; Remennikov, A.; and Sheikh, M. N., “Experimental Investigation of the Behaviour of Concrete Beams Reinforced with GFRP Bars Under Static and Impact Loading,” Engineering Structures, V. 113, Apr. 2016, pp. 220-232. doi: 10.1016/j.engstruct.2016.01.044
16. Jin, L.; Zheng, M.; Zhang, R.; and Du, X., “Investigation on the Impact Response of Concrete Beams Reinforced with Hybrid Steel–BFRP Bars,” Journal of Composites for Construction, ASCE, V. 27, No. 4, Aug. 2023, p. 04023029. doi: 10.1061/JCCOF2.CCENG-4185
17. Ozturk, B.; Senturk, T.; and Yilmaz, C., “Analytical Investigation of Effect of Retrofit Application Using CFRP on Seismic Behavior of a Monumental Building at Historical Cappadocia Region of Turkey,” Proceedings of the 9th U.S. National and 10th Canadian Conference on Earthquake Engineering (9USN/10CCEE): Reaching Beyond Borders, Toronto, ON, Canada, July 2010, Paper No. 186, pp. 2055-2064.
18. Huang, Z.; Chen, W.; Hao, H.; Chen, Z.; Pham, T. M.; Tran, T. T.; and Elchalakani, M., “Flexural Behaviour of Ambient Cured Geopolymer Concrete Beams Reinforced with BFRP Bars Under Static and Impact Loads,” Composite Structures, V. 261, Apr. 2021, Article No. 113282. doi: 10.1016/j.compstruct.2020.113282
19. Liang, X., and Yin, S.-P., “Flexural Durability of Seawater Coral Aggregate Concrete Beams Reinforced with Basalt FRP Bars,” Journal of Composites for Construction, ASCE, V. 26, No. 2, Apr. 2022, p. 04022010. doi: 10.1061/(ASCE)CC.1943-5614.0001201
20. Dong, Z.; Wu, G.; Zhao, X.-L.; Zhu, H.; and Lian, J.-L., “Durability Test on the Flexural Performance of Seawater Sea-Sand Concrete Beams Completely Reinforced with FRP Bars,” Construction and Building Materials, V. 192, Dec. 2018, pp. 671-682. doi: 10.1016/j.conbuildmat.2018.10.166
21. Li, J.; Zhang, R.; Jin, L.; Lan, D.; Zheng, M.; and Du, X., “Effect of Stirrup Ratio on Impact Response of BFRP-Reinforced Concrete Beams Under Different Energy Levels,” International Journal of Impact Engineering, V. 173, Mar. 2023, Article No. 104472. doi: 10.1016/j.ijimpeng.2022.104472
22. Echeverria, C.; Pahlevani, F.; Gaikwad, V.; and Sahajwalla, V., “The Effect of Microstructure, Filler Load and Surface Adhesion of Marine Bio-Fillers, in the Performance of Hybrid Wood-Polypropylene Particulate Bio-Composite,” Journal of Cleaner Production, V. 154, June 2017, pp. 284-294. doi: 10.1016/j.jclepro.2017.04.020
23. Guo, S.; Hu, J.; and Dai, Q., “A Critical Review on the Performance of Portland Cement Concrete with Recycled Organic Components,” Journal of Cleaner Production, V. 188, July 2018, pp. 92-112. doi: 10.1016/j.jclepro.2018.03.244
24. Huang, Z.; Chen, W.; Tran, T. T.; Pham, T. M.; Hao, H.; Chen, Z.; and Elchalakani, M., “Experimental and Numerical Study on Concrete Beams Reinforced with Basalt FRP Bars Under Static and Impact Loads,” Composite Structures, V. 263, May 2021, Article No. 113648. doi: 10.1016/j.compstruct.2021.113648
25. Deng, J.; Pan, Z.; Mai, G.; Long, Y.; Kuang, B.; Zhu, J.; Guo, Q.; Liang, J.; Huang, F.; Qiao, S.; Li, X.; and Liu, F., “Fatigue Behaviour of CFRP Bar-Reinforced Seawater Sea Sand Concrete Beams: Deformation Analysis and Prediction,” Buildings, V. 13, No. 9, 2023, Article No. 2273. doi: 10.3390/buildings13092273
26. Li, S.; Guo, S.; Yao, Y.; Jin, Z.; Shi, C.; and Zhu, D., “The Effects of Aging in Seawater and SWSSC and Strain Rate on the Tensile Performance of GFRP/BFRP Composites: A Critical Review,” Construction and Building Materials, V. 282, May 2021, Article No. 122534. doi: 10.1016/j.conbuildmat.2021.122534
27. Xu, X.; Rawat, P.; Shi, Y.; and Zhu, D., “Tensile Mechanical Properties of Basalt Fiber Reinforced Polymer Tendons at Low to Intermediate Strain Rates,” Composites Part B: Engineering, V. 177, Nov. 2019, Article No. 107442. doi: 10.1016/j.compositesb.2019.107442
28. Cusatis, G., “Strain-Rate Effects on Concrete Behavior,” International Journal of Impact Engineering, V. 38, No. 4, Apr. 2011, pp. 162-170. doi: 10.1016/j.ijimpeng.2010.10.030
29. Yu, Q.; Zhuang, W.; and Shi, C., “Research Progress on the Dynamic Compressive Properties of Ultra-High Performance Concrete Under High Strain Rates,” Cement and Concrete Composites, V. 124, Nov. 2021, Article No. 104258. doi: 10.1016/j.cemconcomp.2021.104258
30. Tran, T. T.; Pham, T. M.; Huang, Z.; Chen, W.; Hao, H.; and Elchalakani, M., “Impact Response of Fibre Reinforced Geopolymer Concrete Beams with BFRP Bars and Stirrups,” Engineering Structures, V. 231, Mar. 2021, Article No. 111785. doi: 10.1016/j.engstruct.2020.111785
31. Kishi, N.; Mikami, H.; Matsuoka, K. G.; and Ando, T., “Impact Behavior of Shear-Failure-Type RC Beams Without Shear Rebar,” International Journal of Impact Engineering, V. 27, No. 9, Oct. 2002, pp. 955-968. doi: 10.1016/S0734-743X(01)00149-X
32. Saleh, Z.; Sheikh, M. N.; Remennikov, A.; and Basu, A., “Overload Damage Mechanisms of GFRP-RC Beams Subjected to High-Intensity Low-Velocity Impact Loads,” Composite Structures, V. 233, Feb. 2020, Article No. 111578. doi: 10.1016/j.compstruct.2019.111578
33. Aminakbari, N.; Kabir, M. Z.; Rahai, A.; and Hosseinnia, A., “Experimental and Numerical Evaluation of GFRP-Reinforced Concrete Beams Under Consecutive Low-Velocity Impact Loading,” International Journal of Civil Engineering, V. 22, No. 1, Jan. 2024, pp. 145-156. doi: 10.1007/s40999-023-00883-9
34. Feng, G.; Zhu, D.; Guo, S.; Rahman, M. Z.; Jin, Z.; and Shi, C., “A Review on Mechanical Properties and Deterioration Mechanisms of FRP Bars Under Severe Environmental and Loading Conditions,” Cement and Concrete Composites, V. 134, Nov. 2022, Article No. 104758. doi: 10.1016/j.cemconcomp.2022.104758
35. Tamai, H.; Sonoda, Y.; and Bolander, J. E., “Impact Resistance of RC Beams with Reinforcement Corrosion: Experimental Observations,” Construction and Building Materials, V. 263, Dec. 2020, Article No. 120638. doi: 10.1016/j.conbuildmat.2020.120638
36. Guo, S.; Xu, Z.; and Zhu, D., “Durability Enhancement of Basalt Fiber-Reinforced Polymer-Seawater Sea-Sand Concrete Beam by Alkalinity Regulation,” ACI Structural Journal, V. 121, No. 4, July 2024, pp. 47-62.
37. Zhu, D.; Zhao, X.; and Guo, S., “Influence of Seawater and Mineral Admixtures on Microstructure and Mechanical Performance of Cement-Based Materials,” Journal of the Chinese Ceramic Society, V. 52, No. 5, 2024, pp. 1477-1485.
38. Li, S.; Zhu, D.; Guo, S.; Yi, Y.; and Feng, G., “Experimental Study on the Effects of Dynamic Loading and Seawater Attack on Bond Behavior Between Basalt Fiber Reinforced Polymer Bars and Seawater Sea-Sand Concrete,” Journal of Building Engineering, V. 72, Aug. 2023, Article No. 106505. doi: 10.1016/j.jobe.2023.106505