Experimental Behavior of Reinforced-Concrete Frames Filled with Reinforced-Concrete Shear Walls (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Behavior of Reinforced-Concrete Frames Filled with Reinforced-Concrete Shear Walls (Prepublished)

Author(s): Erato Oikonomopoulou, Vasiliki Palieraki, Elizabeth Vintzileou, Giovacchino Genesio

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: post-installed connectors; reinforced concrete interfaces; seismic retrofit; shear walls

DOI: 10.14359/51749165

Date: 9/10/2025

Abstract:
Filling reinforced concrete (RC) frame spans with RC shear walls constitutes a strategic intervention to existing sub-standard buildings. The efficiency of this intervention depends, among other things, on the behavior of interfaces between the shear wall and the frame elements. The failure of critical interfaces that may lead to undesirable shear sliding of the wall at its base can only be prevented if the interfaces are adequately designed. To investigate the cyclic behavior of interfaces within the composite frame-to-wall members, four frames filled with RC walls, as well as two reference specimens (i.e., a bare frame and a monolithic frame/wall specimen), were subjected to cyclic horizontal displacements. The crucial effect of the interface reinforcement ratio, the detailing, the dowel distribution along the interface, and the embedment length on the behavior of the specimens, in terms of maximum capacity, drift, and failure mode, was confirmed.