Abstract:
This is the first article in a series of articles prepared by members of ACI Committee 562, Evaluation, Repair, and Rehabilitation of Concrete Structures, under the main theme, “Existing Concrete Structures—Learning Lessons and Advancing Solutions.” It focuses on the evolution of ACI CODE-562 since its first publication as a provisional standard in 2012 to the 2025 edition.

Related References:

1. ACI Committee 562, “Assessment, Repair, and Rehabilitation of Existing Concrete Structures—Code Requirements and Commentary (ACI CODE-562-25),” American Concrete Institute, Farmington Hills, MI, 2025, 130 pp.

2. Kesner, K., and Poston, R.W., “Evolution of ACI 562 Code—Part 5,” Concrete International, V. 38, No. 6, June 2016, pp. 25-27.

3. ACI Foundation, “Vision 2020: A Vision for the Concrete Repair, Protection and Strengthening Industry,” ACI Strategic Development Council, Farmington Hills, MI, 2006, 29 pp.

4. McDonald, J.E., and Campbell, R.L. Sr., “The Condition of Corps of Engineers Civil Works Concrete Structures,” Technical Report REMR-CS-2, U.S. Army Corps of Engineers Waterways Experiment Station, Vicksburg, MS, 1985, 133 pp.

5. Tilly, G.P., and Jacobs, J., Concrete Repairs: Performance in Service and Current Practice, IHS BRE Press, Bracknell, UK, 2007, 44 pp.

6. ACI Innovation Task Group (ITG) 11, “Statistical Techniques for Assessment of Existing Concrete Structures—Report (ACI PRC-ITG-11-24),” American Concrete Institute, Farmington Hills, MI, 2024, 47 pp.

7. Barlow, P.; Triandafilou, N.R.; and Bartlett, F.M., “New ACI Document on Statistical Techniques for Assessment of Existing Concrete Structures,” Concrete International, V. 47, No. 4, Apr. 2025, pp. 41-46.

8. AASHTO, “The Manual for Bridge Evaluation, 2022 Interim Revisions,” third edition, American Association of State Highway and Transportation Officials, Washington, DC, 2018, 749 pp.

9. AREMA, “Bridge Inspection Handbook,” second edition, American Railway Engineering and Maintenance-of-Way Association, Lanham, MD, 2017, 355 pp.

10. SEI/ASCE 11-99, “Guideline for Structural Condition Assessment of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2000, 147 pp.