On Concrete Properties during Heating and Cooling

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: On Concrete Properties during Heating and Cooling

Author(s): Patrick Bamonte, Fabienne Robert, and Thomas Gernay

Publication: Materials Journal

Volume: 122

Issue: 6

Appears on pages(s): 5-16

Keywords: compressive strength; fire; high temperature; hot tests; residual tests; thermal diffusivity

DOI: 10.14359/51749132

Date: 11/1/2025

Abstract:
The use of parametric/natural fires in the design of reinforced concrete structures in fire conditions requires an accurate definition of the temperature-induced evolution of the thermal and mechanical properties. Within this context, the characterization of four normal-strength concretes (fc20 = 4200 to 6800 psi [29 to 47 MPa]), with siliceous and carbonate aggregates, are studied herein concerning the thermal diffusivity D (between 68 and 1652°F [20 and 900°C]) and under uniaxial compression after different thermal cycles, with reference maximum temperatures of 392, 752, and 1112°F (200, 400, and 600°C). The results show that thermal diffusivity exhibits mostly irreversible behavior after exposure to temperatures over 1382°F (750°C). Concerning the compressive strength, the hot and residual values (when Ttest = 68°F [20°C]) are, overall, in line with the most common standard provisions. Quite interestingly, the tests carried out at intermediate temperatures (with Ttest ≠ Tmax and Ttest > 68°F [20°C]) highlighted a strength decay, which is not simply an interpolation between hot and residual values.

Related References:

1. Bažant, Z. P., and Kaplan, M. F., Concrete at High Temperatures—Material Properties and Mathematical Models, Longman Group Limited, London, UK, 1996, 412 pp.

2. Khoury, G. A., “Effect of Fire on Concrete and Concrete Structures,” Progress in Structural Engineering and Materials, V. 2, No. 4, 2000, pp. 429-447. doi: 10.1002/pse.51

3. “Fire in the Windsor Building, Madrid. Survey of the Fire Resistance and the Residual Bearing Capacity of the Structure after the Fire,” INTEMAC, NIT 2-05, Dec. 2005.

4. Felicetti, R., and Gambarova, P. G., “Effects of High Temperature on the Residual Compressive Strength of High-Strength Siliceous Concretes,” ACI Materials Journal, V. 95, No. 4, July-Aug. 1998, pp. 395-406.

5. Torelli, G.; Mandal, P.; Gillie, M.; and Tran, V.-X., “A Confinement-Dependent Load-Induced Thermal Strain Constitutive Model for Concrete Subjected to Temperatures Up to 500 °C,” International Journal of Mechanical Sciences, V. 144, Aug. 2018, pp. 887-896. doi: 10.1016/j.ijmecsci.2017.12.054

6. Bamonte, P., and Gambarova, P. G., “Properties of Concrete Required in Nuclear Power Plants,” Infrastructure Systems for Nuclear Energy, John Wiley & Sons Ltd, Chichester, UK, 2014, pp. 407-438.

7. Malhotra, H. L., “Effect of Temperature on the Compressive Strength of Concrete,” Magazine of Concrete Research, V. 8, No. 23, 1956, pp. 85-94. doi: 10.1680/macr.1956.8.23.85

8. Harmathy, T. Z., “Effect of Moisture on the Fire Endurance in Building Materials,” Moisture in Materials in Relation to Fire Tests, No. 385, 1965, pp. 74-95. doi: 10.1520/STP48429S

9. Abrams, M. S., “Compressive Strength of Concrete at Temperatures to 1600 F,” Temperature and Concrete, ACI SP-25, American Concrete Institute, Farmington Hills, MI, 1971.

10. Anderberg, J., and Thelandersson, S., “Stress and Deformation Characteristics of Concrete at High Temperatures,” Bulletin 54, Lund Institute of Technology, Lund, Sweden, 1976.

11. Naus, D. J.; Oland, C. B.; and Robinson, G. C., “Testing Program for Concrete at Temperatures to 894 K,” Transactions, 6th SMiRT International Conference, Paris, France, 1981.

12. Thelandersson, S., “On the Multiaxial Behavior of Concrete Exposed to High Temperature,” Nuclear Engineering and Design, V. 75, No. 2, 1982, pp. 271-282. doi: 10.1016/0029-5493(83)90023-7

13. Khoury, G. A., “Compressive Strength of Concrete at High Temperatures: A Reassessment,” Magazine of Concrete Research, V. 44, No. 161, 1992, pp. 291-309. doi: 10.1680/macr.1992.44.161.291

14. RILEM-Committee 44-PHT, “Behavior of Concrete at High Temperatures,” U. Schneider, ed., Kassel University, Kassel, Germany, 1985, 122 pp.

15. Papayianni, J., and Valiasis, T., “Residual Mechanical Properties of Heated Concrete Incorporating Different Pozzolanic Materials,” Materials and Structures, V. 24, No. 2, 1991, pp. 115-121. doi: 10.1007/BF02472472

16. Takeuchi, M.; Hiramoto, M.; Kumagai, N.; Yamazaki, N.; Kodaira, A.; and Sugiyama, K., “Materials Properties of Concrete and Steel Bars at Elevated Temperatures,” Transactions, 12th SMiRT International Conference, Stuttgart, Germany, 1993.

17. Anand, N.; Thanaraj, D. P.; Andrushia, D.; Lublóy, É. E.; Kiran, T.; Kanagaraj, B.; and Kodur, V., “Microstructure Investigation, Strength Assessment, and Thermal Modelling of Concrete Exposed to Different Heating Cooling Regimes,” Journal of Thermal Analysis and Calorimetry, V. 148, No. 9, 2023, pp. 3221-3247. doi: 10.1007/s10973-023-11998-5

18. Liu, K.; Liu, J.; Li, J.; Tao, M.; and Wu, C., “Experimental Investigation of Heating-Cooling Effects on the Mechanical Properties of Geopolymer-Based High Performance Concrete Heated to Elevated Temperatures,” Structures, V. 47, Jan. 2023, pp. 735-747. doi: 10.1016/j.istruc.2022.11.097

19. EN 1992-1-2:2004, “Eurocode 2: Design of Concrete Structures - Part 1-2: General Rules - Structural Fire Design,” European Committee for Standardization, Brussels, Belgium, 2004.

20. EN 1994-1-2:2005, “Eurocode 4: Design of Composite Steel and Concrete Structures - Part 1-2: General Rules - Structural Fire Design,” European Committee for Standardization, Brussels, Belgium, 2005.

21. ACI Committee 216, “Code Requirements for Determining Fire Resistance of Concrete and Masonry Construction Assemblies (ACI 216.1-07),” American Concrete Institute, Farmington Hills, MI, 2007, 32 pp.

22. Diederichs, U.; Jumppanen, U. M.; and Penttala, V., “Material Properties of High-Strength Concrete at Elevated Temperatures,” Transactions, 13th IABSE Congress, Helsinki, Finland, 1988, pp. 489-494.

23. Diederichs, U.; Jumppanen, U. M.; and Penttala, V., “Behavior of High-Strength Concrete at High Temperatures,” Report No. 92, Helsinki University of Technology, Helsinki, Finland, 1989, 76 pp.

24. FIP-CEB, “High-Strength Concrete: State of the Art Report,” Bulletin d’Information No. 197, Working Group on “High-Strength Concrete,” 1990, 61 pp.

25. Law, A., and Hadden, R., “Burnout Means Burnout,” SFPE Europe Magazine, Issue 5, 2017, 4 pp.

26. Law, A., and Bisby, L., “The Rise and Rise of Fire Resistance,” Fire Safety Journal, V. 116, 2020, p. 103188. doi: 10.1016/j.firesaf.2020.103188

27. Gernay, T., and Franssen, J.-M., “A Performance Indicator for Structures under Natural Fire,” Engineering Structures, V. 100, 2015, pp. 94-103. doi: 10.1016/j.engstruct.2015.06.005

28. Bamonte, P.; Kalaba, N.; and Felicetti, R., “Computational Study on Prestressed Concrete Members Exposed to Natural Fires,” Fire Safety Journal, V. 97, 2018, pp. 54-65. doi: 10.1016/j.firesaf.2018.02.006

29. Gernay, T., “Fire Resistance and Burnout Resistance of Reinforced Concrete Columns,” Fire Safety Journal, V. 104, 2019, pp. 67-78. doi: 10.1016/j.firesaf.2019.01.007

30. Lo Monte, F.; Bamonte, P.; and Beltrami, C., “Study on the Effects of Cooling Phase and Construction Technology on the Fire Performance of R/C Tunnels,” Tunnelling and Underground Space Technology, V. 132, 2023, p. 104838. doi: 10.1016/j.tust.2022.104838

31. Gernay, T.; Franssen, J.-M.; Robert, F.; McNamee, R.; Felicetti, R.; Bamonte, P.; Brunkhorst, S.; Mohaine, S.; and Zehfuß, J., “Experimental Investigation of Structural Failure during the Cooling Phase of a Fire: Concrete Columns,” Fire Safety Journal, V. 134, 2022, p. 103691. doi: 10.1016/j.firesaf.2022.103691

32. Hua, N.; Khorasani, N. E.; Tessari, A.; and Ranade, R., “Experimental Study of Fire Damage to Reinforced Concrete Tunnel Slabs,” Fire Safety Journal, V. 127, 2022, p. 103504. doi: 10.1016/j.firesaf.2021.103504

33. Wright, S., and Redmond, L., “Methodology for Predicting Concrete Strength after Short-Term Heat Exposure,” ACI Materials Journal, V. 120, No. 6, Nov. 2023, pp. 33-46.

34. Gernay, T.; Pei, J.; Tong, Q.; and Bamonte, P., “Numerical Analysis of the Effects of Fire with Cooling Phase on Reinforced Concrete Members,” Engineering Structures, V. 293, 2023, p. 116618. doi: 10.1016/j.engstruct.2023.116618

35. Neville, A. M., and Brooks, J. J., Concrete Technology, second edition, Pearson Education Limited, Edinburgh, UK, 442 pp.

36. EN 1992-1-1:2004, “Eurocode 2: Design of Concrete Structures - Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004.

37. Khoury, G. A.; Sullivan, J. E.; and Grainger, B. N., “Radial Temperature Distributions within Solid Concrete Cylinders under Transient Thermal States,” Magazine of Concrete Research, V. 36, No. 128, 1984, pp. 146-154. doi: 10.1680/macr.1984.36.128.146

38. Klingsch, E.; Frangi, A.; and Fontana, M., “Residual Strength of Thermally-Damaged Concrete: Blended Cement Versus Ordinary Portland Cement,” Studies and Researches, V. 29, 2009, pp. 131-154.


ALSO AVAILABLE IN:

Electronic Materials Journal