Allowable Capacities of Power-Actuated Fasteners in Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Allowable Capacities of Power-Actuated Fasteners in Concrete

Author(s): F. Michael Bartlett, Peter Grzesik, and Christopher Gill

Publication: Structural Journal

Volume: 123

Issue: 1

Appears on pages(s): 3-14

Keywords: abrasion and impact resistance; aggregate; factor of safety; lightweight concrete; Monte Carlo simulation; normalweight concrete; power-actuated fastener (PAF); reliability; working-stress design

DOI: 10.14359/51749130

Date: 1/1/2026

Abstract:
This paper proposes new procedures for determining allowable loads for power-actuated fasteners that are consistent with ASCE/SEI 7-22. Thirty new load test data sets for single fasteners in shear and tension and fastener groups in shear are analyzed statistically. The current ICC-ES AC70-2021 procedure yields allowable loads that are quite variable, even negative, and very sensitive to “reject-as-outlier” decisions. In addition, ICC-ES AC70 procedures to determine allowable loads can currently not be clearly linked to the reliability requirements of ASCE/SEI 7-22. Monte Carlo simulation demonstrates that the proposed simplified method, derived from the described detailed method, is robust for sample sizes as small as 10 specimens. It yields allowable fastener loads that are 10 to 25% greater than those obtained using the current ICC-ES AC70 procedure yet are typically 60 to 90% of the actual allowable fastener loads, derived from the described detailed method to assess allowable loads in line with ASCE/SEI 7-22 reliability requirements. The new provisions are extended to cases where the coarse aggregate hardness in the test specimens differs from that in the structure, which is not addressed in ICC-ES AC70.

Related References:

1. ICC-ES AC70, “Acceptance Criteria for Power-Actuated Fasteners Driven into Concrete, Steel and Masonry Elements,” International Code Council Evaluation Service, Brea, CA, 2021, 18 pp.

2. ASTM E1190-21, “Standard Test Methods for Strength of Power-Actuated Fasteners Installed in Structural Members,” ASTM International, West Conshohocken, PA, 2021, 6 pp.

3. ASTM C33/C33M-18, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2018, 8 pp.

4. ASTM C330/C330M-17a, “Standard Specification for Lightweight Aggregates for Structural Concrete,” ASTM International, West Conshohocken, PA, 2017, 4 pp.

5. ASCE/SEI 7-22, “Minimum Design Loads and Associated Criteria for Buildings and Other Structures,” American Society of Civil Engineers, Reston, VA, 2022, 1072 pp.

6. Hilti, “Instructions for Use Hilti X-CX ALH ceiling hangers, Status 05-2018”, Hilti Corporation, Schaan, Liechtenstein, 2018, https://productdata.hilti.com/APQ_HC_RAW/PUB_5338814_000.pdf?_gl=1*kb5ocq*_gcl_au*NTExMjExNDAwLjE3NjM5ODQ4NzM.*_ga*MTg1MTUwNzQ5OC4xNzYzOTg0ODc0*_ga_EWPGKCHLCH*czE3NjM5ODQ4NzMkbzEkZzEkdDE3NjM5ODQ5NzUkajU5JGwwJGgw. (last accessed Dec. 1, 2025)

7. Applied Testing & Geosciences, “Test Report E1190-030818-12381-4368,” Applied Testing & Geosciences, LLC, Bridgeport, PA, 2018.

8. CEL Consulting, “Test Report 18H388,” CEL Consulting, Oakland, CA, 2018.

9. Element Materials Technology, “Test Report No. ESP027823P1.R0,” St. Paul, MN, 2018.

10. Progressive Engineering Inc., “Test Report 2017-6231,” Goshen, IN, 2018.

11. Element Materials Technology, “Test Report No. ESP032240P.1R0,” St. Paul, MN, 2020.

12. Element Materials Technology, “Test Report No. ESP032240P.2R0,” St. Paul, MN, 2020.

13. Specialized Testing, Inc., “Test Report No. STQA50750.1R0,” Santa Fe Springs, CA, 2020.

14. Specialized Testing, Inc., “Test Report No. STQA50750.2R0,” Santa Fe Springs, CA, 2020.

15. Overacker, S. D., “Variations in Power-Actuated Fastener Shear Capacity with Respect to Concrete Coarse Aggregate Properties,” MSc thesis, University of Minnesota Twin Cities, Minneapolis, MN, 2019, 306 pp.

16. Larsen, R. J., and Marx, M. L., An Introduction to Mathematical Statistics and Its Applications, sixth edition, Prentice Hall, Upper Saddle River, NJ, 2017, 752 pp.

17. CSA S408-11, “Guidelines for the Development of Limit States Design Standards,” CSA Group, Toronto, ON, 2011, 62 pp.

18. Ellingwood, B.; Galambos, T. V.; MacGregor, J. G.; and Cornell, C. A., “Development of a Probability Based Load Criterion for American National Standard A58: Building Code Requirements for Minimum Design Loads in Buildings and Other Structures,” NBS Special Publication 577, U.S. Department of Commerce, National Institute of Standards and Technology, Gaithersburg, MD, 1980, 236 pp.

19. McAllister, T. P.; Wang, N.; and Ellingwood, B. R., “Risk-Informed Mean Recurrence Intervals for Updated Wind Maps in ASCE 7-16,” Journal of Structural Engineering, ASCE, V. 144, No. 5, May 2018, p. 06018001. doi: 10.1061/(ASCE)ST.1943-541X.0002011

20. ACI Committee 214, “Obtaining Cores and Interpreting Core Compressive Strength Results—Guide (ACI PRC-214.4-21),” American Concrete Institute, Farmington Hills, MI, 2021, 20 pp.

21. Bartlett, F. M., Allowable Tension and Shear Capacities of Power-Actuated Fasteners in Concrete, Report for Hilti USA, 2023, 60 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal