Determining When Drilled Shafts Are Mass Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Determining When Drilled Shafts Are Mass Concrete

Author(s): Amanda Lewis, Kevin Johnson, Abla Zayed, and Gray Mullins

Publication: Materials Journal

Volume: 122

Issue: 6

Appears on pages(s): 59-72

Keywords: drilled shaft; mass concrete; thermal integrity profiling; thermal modeling

DOI: 10.14359/51749125

Date: 11/1/2025

Abstract:
The term “mass concrete” characterizes a specific concrete condition that typically requires unique considerations to mitigate extreme temperature effects on a structure. Mass concrete has historically been defined by the physical dimensions of a massive concrete element with the intent of identifying when differential temperatures may induce early-onset cracking, leading to reduced service life. More recently, in addition to differential temperature considerations, extreme upper temperature limits have been imposed by the American Concrete Institute to prevent long-term concrete degradation. Studies dating back to 2007 show that shafts as small as 48 in. (1.2 m) in diameter can exceed both differential and peak temperature limits; in 2020, augered cast-in-place piles as small as 30 in. (0.76 m) in diameter exceeded one or both limits. This suggests the term “mass concrete” is misleading when considering today’s high-early-strength or high-performance mixture designs. This study applies numerical modeling coupled with field measurements to investigate the effects of concrete mixture design, drilled shaft diameter, and environmental conditions on heat energy production and temperature. Further, the outcome of this study focuses on developing criteria that combine the effects of both size and cementitious material content to determine whether unsafe temperature conditions may arise for a given drilled shaft design.

Related References:

1. Gunaratne, M., The Foundation Engineering Handbook, CRC Press, Boca Raton, FL, 2014.

2. ACI Committee 201, “Durable Concrete—Guide (ACI PRC-201.2-23),” American Concrete Institute, Farmington Hills, MI, 2023, 99 pp.

3. ACI Committee 301, “Specifications for Structural Concrete (ACI 301-16),” American Concrete Institute, Farmington Hills, MI, 2016, 64 pp.

4. COMSOL, “COMSOL Multiphysics Simulation Software,” COMSOL, Inc., Burlington, MA, 2024.

5. ACI Committee 207, “Report on Thermal and Volume Change Effects on Cracking of Mass Concrete (ACI 207.2R-07),” American Concrete Institute, Farmington Hills, MI, 2007, 28 pp.

6. FDOT, “Standard Specifications for Road and Bridge Construction – Section 346-3.3: Mass Concrete,” Florida Department of Transportation, Tallahassee, FL, 2019.

7. FDOT, “Structures Design Guidelines,” Florida Department of Transportation, Tallahassee, FL, 2019.

8. AASHTO, “AASHTO LRFD Bridge Construction Specification, 4th ed., 2024 Interim Revisions,” American Association of State Highway and Transportation Officials, Washington, DC, 2024.

9. ASTM D7949-25, “Standard Test Methods for Thermal Integrity Profiling of Concrete Deep Foundations,” ASTM International, West Conshohocken, PA, 2025.

10. Mullins, G., “Thermal Integrity Profiling of Drilled Shafts,” The Journal of the Deep Foundations Institute, V. 4, No. 2, 2010, pp. 54-64.

11. Mullins, G.; Johnson, K.; Winters, D.; Hilferding, H.; and Kupselaitis, K., “Selection of Thermal Integrity Data Regression Parameters,” Geotechnical Testing Journal, V. 44, No. 3, 2021, pp. 741-755. doi: 10.1520/GTJ20190084

12. ACI, “ACI Concrete Terminology (ACI CT-21),” American Concrete Institute, Farmington Hills, MI, 2021, 80 pp.

13. ACI Committee 224, “Control of Cracking in Concrete Structures (ACI 224R-01),” American Concrete Institute, Farmington Hills, MI, 2001, 46 pp.

14. ACI Committee 207, “Mass Concrete—Guide (ACI PRC-207.1-21),” American Concrete Institute, Farmington Hills, MI, 2021, 34 pp.

15. ACI Committee 308, “Guide to External Curing of Concrete (ACI 308R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 36 pp.

16. Zhu, H.; Mapa, D. G.; Lucero, C.; Riding, K. A.; and Zayed, A., “Effect of Slag Characteristics on Adiabatic Temperature Rise of Blended Concrete,” ACI Materials Journal, V. 119, No. 1, Jan. 2022, pp. 117-131.

17. Zayed, A.; Riding, K. A.; Stetsko, Y.; Shanahan, N.; Markandeya, A.; Nosouhian, F.; Mapa, D.; and Fincan, M., “Effects of Blast Furnace Slag Characteristics on Durability of Cementitious Systems for Florida Concrete Structures,” FDOT Project BDV25-977-28, Florida Department of Transportation, Tallahassee, FL, 2019.

18. IDOT, “Standard Specifications for Road and Bridge Construction,” Illinois Department of Transportation, Springfield, IL, 2016.

19. Mee, T., “Quality Assurance of Cast-in-Place Foundation Elements,” doctoral dissertation, University of South Florida, Tampa, FL, 2024.

20. DelDOT, “Standard Specifications for Road and Bridge Construction,” Delaware Department of Transportation, Dover, DE, 2022.

21. Iowa DOT, “Standard Specifications for Highway and Bridge Construction,” Iowa Department of Transportation, Ames, IA, 2023.

22. MnDOT, “2020 SB Bridge Special Provisions, Revised July 2024,” Minnesota Department of Transportation, St. Paul, MN, 2024.

23. NDDOT, “Standard Specifications for Road and Bridge Construction,” North Dakota Department of Transportation, Bismarck, ND, 2023.

24. NYSDOT, “Standard Specifications, Volume 4 Construction and Materials,” New York Department of Transportation, Albany, NY, 2021.

25. ALDOT, “Standard Specifications for Highway Construction,” Alabama Department of Transportation, Montgomery, AL, 2022.

26. AKDOT, “Standard Specifications for Highway Construction,” Alaska Department of Transportation and Public Facilities, Juneau, AK, 2020.

27. ADOT, “Standard Specifications for Road and Bridge Construction,” Arizona Department of Transportation, Phoenix, AZ, 2021.

28. ARDOT, “Standard Specifications for Highway Construction,” Arkansas Department of Transportation, Little Rock, AR, 2014.

29. Caltrans, “Standard Specifications, 2023 Edition,” California State Transportation Agency, California Department of Transportation, Sacramento, CA, 2023.

30. CDOT, “Standard Specifications for Road and Bridge Construction,” Colorado Department of Transportation, Denver, CO, 2022.

31. CTDOT, “Bridge Design Manual,” Connecticut Department of Transportation, Newington, CT, 2003.

32. GDOT, “Standard Specifications Construction of Transportation Systems,” Georgia Department of Transportation, Atlanta, GA, 2021.

33. HDOT, “2005 Standard Specifications,” Hawaii Department of Transportation, Highways, Honolulu, HI, 2005.

34. ITD, “Standard Specifications for Highway Construction,” Idaho Transportation Department, Boise, ID, 2018.

35. INDOT, “Standard Specifications,” Indiana Department of Transportation, Indianapolis, IN, 2020.

36. KYTC, “Standard Specifications for Road and Bridge Construction,” Kentucky Transportation Cabinet, Frankfort, KY, 2019.

37. LaDOTD, “Louisiana Standard Specifications for Roads and Bridges,” Louisiana Department of Transportation and Development, Baton Rouge, LA, 2016.

38. MaineDOT, “Department of Transportation Standard Specifications,” Maine Department of Transportation, Augusta, ME, 2020.

39. MDOT, “Standard Specifications for Construction and Materials,” Maryland Department of Transportation State Highway Administration, Baltimore, MD, 2023.

40. MassDOT, “Standard Specifications for Highways and Bridges,” Massachusetts Department of Transportation, Boston, MA, 2023.

41. MDOT, “Standard Specifications for Construction,” Michigan Department of Transportation, Lansing, MI, 2020.

42. MoDOT, “Standard Specifications for Highway Construction,” Missouri Highways and Transportation Commission, Jefferson City, MO, 2024.

43. MDT, “Standard Specifications for Road and Bridge Construction,” Montana Department of Transportation, Billings, MT, 2024.

44. NDOT, “Standard Specifications for Highway Construction,” Nebraska Department of Transportation, Lincoln, NE, 2017.

45. NDOT, “Standard Specifications for Road and Bridge Construction,” Nevada Department of Transportation, Carson City, NV, 2014.

46. NJDOT, “Standard Specifications for Road and Bridge Construction,” New Jersey Department of Transportation, Trenton, NJ, 2019.

47. NMDOT, “Standard Specifications for Highway and Bridge Construction,” New Mexico Department of Transportation, Santa Fe, NM, 2019.

48. NCDOT, “Standard Specifications for Roads and Structures,” North Carolina Department of Transportation, Raleigh, NC, 2018.

49. ODOT, “Construction and Materials Specifications,” Ohio Department of Transportation, Columbus, OH, 2024.

50. ODOT, “Standard Specifications for Highway Construction,” Oklahoma Department of Transportation, Oklahoma City, OK, 2019.

51. ODOT, “Standard Specifications for Construction,” Oregon Department of Transportation, Salem, OR, 2024.

52. PennDOT, “Specifications,” Pennsylvania Department of Transportation, Harrisburg, PA, 2005.

53. RIDOT, “Standard Specifications for Road and Bridge Construction,” Rhode Island Department of Transportation, Providence, RI, 2018.

54. SCDOT, “Standard Specifications for Highway Construction,” South Carolina Department of Transportation, Columbia, SC, 2007.

55. SDDOT, “Standard Specifications for Roads and Bridges,” South Dakota Department of Transportation, Pierre, SD, 2015.

56. TDOT, “Standard Specifications for Road and Bridge Construction,” Tennessee Department of Transportation, Nashville, TN, 2021.

57. TxDOT, “Standard Specifications for Construction and Maintenance of Highways, Streets, and Bridges,” Texas Department of Transportation, Austin, TX, 2024.

58. UDOT, “Standard Specifications for Road and Bridge Construction,” Utah Department of Transportation, Salt Lake City, UT, 2024.

59. VTrans, “Standard Specifications for Construction,” Vermont Agency of Transportation, Barre, VT, 2024.

60. VDOT, “Road and Bridge Specifications,” Virginia Department of Transportation, Richmond, VA, 2020.

61. WSDOT, “Standard Specifications for Road, Bridge, and Municipal Construction,” Washington State Department of Transportation, Olympia, WA, 2024.

62. WVDOH, “Standard Specifications for Roads and Bridges,” West Virginia Department of Transportation, Division of Highways, Charleston, WV, 2023.

63. WisDOT, “Standard Specifications, Part 5-Structures,” Wisconsin Department of Transportation, Madison, WI, 2024.

64. WYDOT, “Standard Specifications for Road and Bridge Construction,” Wyoming Department of Transportation, Cheyenne, WY, 2021.

65. Mullins, G., and Kranc, S., “Thermal Integrity Testing of Drilled Shafts, Final Report,” Florida Department of Transportation, Tallahassee, FL, 2007.

66. Mullins, G., Ongoing Unpublished Test Results from FDOT Construction in South Florida, 2021.

67. Mlakar, P. F.; Corley, W. G.; Sozen, M. A.; and Thornton, C. H., “The Oklahoma City Bombing: Analysis of Blast Damage to the Murrah Building,” Journal of Performance of Constructed Facilities, V. 12, No. 3, 1998, pp. 100-112.

68. Steel, B. W., “Mass Concrete Research for Hoover Dam,” ACI Journal Proceedings, V. 29, Mar.-Apr. 1933, pp. 305-317.

69. Blanks, R. F.; Meissner, H. S.; and Rawhouser, C., “Cracking in Mass Concrete,” ACI Journal Proceedings, V. 34, No. 3, Mar. 1938, pp. 477-495.

70. Bogue, R. H., “Calculation of the Compounds in Portland Cement,” American Chemical Society,” Industrial and Engineering Chemistry. Analytical Edition, V. 1, No. 4, Oct. 1929, pp. 192-197.

71. Lerch, W., and Bogue, R. H., “Heat of Hydration of Portland Cements,” U.S. Department of Commerce,” Bureau of Standards Journal of Research, V. 12, 1934, pp. 645-664.

72. Rawhouser, C., “Cracking and Temperature Control of Mass Concrete,” ACI Journal Proceedings, V. 41, No. 2, Feb. 1945, pp. 305-346.

73. Riding, A. K.; Poole, J. L.; Folliard, K. J.; Juenger, M. C. G.; and Schindler, A. K., “Modeling Hydration of Cementitious Systems,” ACI Materials Journal, V. 109, No. 2, Mar.-Apr. 2012, pp. 225-234.

74. Bogue, R. H., The Chemistry of Portland Cement, Reinhold Publishing Corporation, New York, 1947, 594 pp.

75. Freiesleben Hansen, P., and Pedersen, E. J., “Maaleinstrument til Kontrol af Betons Haerdning (Maturity Computer for Controlled Curing and Hardening of Concrete),” Nordisk Betong, No. 1, 1977, pp. 21-25.

76. Freiesleben Hansen, P., and Pedersen, E. J., “Curing of Concrete Structures,” European Committee for Concrete, Draft CEB Guide to Durable Concrete Structures, Information Bulletin No. 166, 1985.

77. Schindler, A. K., “Effect of Temperature on Hydration of Cementitious Materials,” ACI Materials Journal, V. 101, No. 1, Jan.-Feb. 2004, pp. 72-81.

78. Schindler, A., and Folliard, K., “Heat of Hydration Models for Cementitious Materials,” ACI Materials Journal, V. 102, No. 1, Jan.-Feb. 2005, pp. 24-33.

79. Folliard, K. J.; Juenger, M.; Schindler, A.; Riding, K.; Poole, J.; Kallivokas, L. F.; Slatnick, S.; Whigham, J.; and Meadows, J. L., “Prediction Model for Concrete Behavior,” Final Report No. FHWA/TX-08/0-4563-1, Texas Department of Transportation, Austin, TX, 2008.

80. Ruiz, J. M.; Rasmussen, R. O.; Chang, G. K.; Dick, J. C.; Nelson, P. K.; Schindler, A. K.; Turner, D. J.; and Wilde, J. W., “Computer-Based Guidelines for Concrete Pavements, Volume III: Technical Appendices,” Report No. FHWA-HRT-04-127, Federal Highway Administration, McLean, VA, 2006, 361 pp.

81. Poole, J. L., “Modeling Temperature Sensitivity and Heat Evolution of Concrete,” PhD dissertation, The University of Texas at Austin, Austin, TX, 2007, 577 pp.

82. Johnson, K. R., “Thermal Integrity Analysis of Concrete Bridge Foundations Using COMSOL Multiphysics® Software,” 2017 COMSOL Conference, Boston, MA, 2017.

83. Idries, A., “Thermal Integrity Profiling (TIP) and Crosshole Sonic Logging (CSL) Testing for Drilled Shafts,” PhD dissertation, University of Illinois Urbana-Champaign, Urbana, IL, 2023.

84. Belardo, D.; Robertson, S.; and Coleman, T., “Instrumentation and Evaluation of Thermal Integrity Profiling Measurements,” Proceedings of the 46th Deep Foundations Institute Annual Conference 2021 (DFI46), Las Vegas, NV, Oct. 2021, pp. 223-236.

85. Coleman, T., and Belardo, D., “Drilled Shaft Base Quality Reductions Identified with Thermal Integrity Profiling,” Proceedings of the 48th Deep Foundations Institute Annual Conference 2023 (DFI48), Seattle, WA, Oct. 2023, pp. 16-28.

86. Mullins, G.; Lewis, A.; Mee, T.; and Vomacka, J., “Peak Temperature Determination of Drilled Shafts Excluded from Mass Concrete Consideration in Current Specifications,” FDOT Project BDV24 977-75, Final Report, Florida Department of Transportation, Tallahassee, FL, 2023.

87. Schindler, A. K.; Dossey, T.; and McCullough, B. F., “Temperature Control During Construction to Improve the Long Term Performance of Portland Cement Concrete Pavements,” Final Report No. FHWA/TX-05/0-1700-2, Texas Department of Transportation, Austin, TX, 2002.

88. Costello, K.; Mobley, S.; Bowen, J.; and Mullins, G., “Reinforcing Bar Pullout Bond in Tremie-Placed Concrete Cast in Drilling Slurry Environments,” ACI Structural Journal, V. 116, No. 4, July 2019, pp. 183-192


ALSO AVAILABLE IN:

Electronic Materials Journal