Title: Structural nanomodified concrete: an investigation of critical properties

Author(s): David J Corr

Publication: CRC

Volume:

Issue:

Appears on pages(s): 11

Keywords:

DOI:

Date: 10/1/2023

Abstract:
The objectives of this project were to investigate long term mechanical and durability characteristics of nanomodified concrete. With the incorporation of well dispersed CNT/CNF it is expected that properties such as creep, shrinkage and corrosion will be influenced. Specifically, at the conclusion of the project, we will have examined: •Creep behavior of CNT/CNF nanomodified concrete •Shrinkage properties of CNT/CNF nanomodified concrete •Corrosion potential of CNT/CNF nanomodified concrete