A Model for Shear Stress of SFRC Beams with Stirrups (Prepublished)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Model for Shear Stress of SFRC Beams with Stirrups (Prepublished)

Author(s): Elielson Sousa and Dênio Oliveira

Publication: Structural Journal

Volume:

Issue:

Appears on pages(s):

Keywords: beam; concrete; shear; steel fibers; stirrups

DOI: 10.14359/51748927

Date: 6/18/2025

Abstract:
Based on statistical analysis, this paper discusses a theoretical model for determining shear strength in steel fiber reinforced concrete beams with transverse reinforcement, using the univariate nonlinear regression of a database consisting of 100 SFRC beams with stirrups, which were analyzed and tested experimentally to shear failure. The proposed model was applied to another database with 150 SFRC beams with transverse reinforcement, which had also experienced shear failure. To check whether the model works for ultimate shear stresses, the effectiveness of the proposed equation was measured by statistically comparing the accuracy of the shear stress values obtained through the model with those acquired through the standard equations and with the experimental values for stress present in the database. These comparisons between the theoretical and experimental results demonstrate that the developed expression efficiently predicts the shear strength of SFRC beams.