Numerical Implementation of an Additive Strain Model for the Damage Simulation of Fatigue‑Loaded Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Numerical Implementation of an Additive Strain Model for the Damage Simulation of Fatigue‑Loaded Concrete

Author(s): Dennis Birkner and Steffen Marx

Publication: IJCSM

Volume: 19

Issue:

Appears on pages(s):

Keywords: Concrete, Damage, Fatigue, FEM, Stress redistribution, ANSYS 1 Introduction One way to reduce global CO2 emissions is to use more renewable energy sources. Wind energy in particular plays an important role in this regard. To increase the energy yield from

DOI: 10.1186/s40069-025-00762-8

Date: 5/31/2025

Abstract:
Investigating the fatigue behavior of concrete structures from wind turbine towers is associated with major challenges due to the high number of occurring load cycles and large cross-sectional dimensions. Thus, only few studies have been carried out on concrete structures subjected to cyclic bending loads. Numerical simulations, in contrast, enable fast investigations of many parameter variations. There are many material models available for different applications, yet they quickly become very complex and require time-consuming calibration of input parameters in structural tests. A model for simulating macroscopic damage processes in fatigue-loaded compressed concrete cross sections, which can be calibrated using standard cylinder tests, does not yet exist. The present work aims to close this gap and implements an additive strain model to simulate the strain and damage development of concrete subjected to fatigue bending loads. Therefore, experimental investigations were designed and carried out. Static and cyclic tests on concrete cylinders yielded the input parameters for the material model. A strain model was implemented in ANSYS Mechanical. The numerical implementation was validated using fatigue tests on large prestressed beams in a resonance- based testing facility. The beam specimens mostly failed due to fatigue in the compression zone. The numerical model confirmed the effects observed in the beam tests and was able to simulate the most damaged regions very well. Moreover, stress redistribution to less loaded regions as a result of relief of the damaged regions was detected. This confirmed the positive effect of stress redistributions on the fatigue life of the structures.