Title:
Advances in Engineered Cementitious Composites: A Comprehensive Review
Author(s):
N. M. Sutan, F. Amsyar Redzuan, A. R. B. A. Karim, N. M. Sa’don, Y. S. S. Hui, and C. C. Y. Jie
Publication:
Materials Journal
Volume:
122
Issue:
4
Appears on pages(s):
111-124
Keywords:
bendable concrete; engineered cementitious composites (ECC); high-performance concrete; hybrid fiber reinforcement; mineral additives; sustainable construction
DOI:
10.14359/51746811
Date:
7/1/2025
Abstract:
Engineered cementitious composites (ECC) represent a significantinnovation in construction materials due to their exceptionalflexibility, tensile strength, and durability, surpassing traditionalconcrete. This review systematically examines the composition,mechanical behavior, and real-world applications of ECC, with afocus on how fiber reinforcement, mineral additives, and micromechanical design improve its structural performances. The present study reports on the effects of various factors, including different types of mineral admixtures, aggregate sizes, fiber hybridization, and specimen dimensions. Key topics include ECC’s strain hardening properties, its sustainability, and its capacity to resist crack development, making it ideal for high-performance infrastructure projects. Additionally, the review discusses recentadvancements in ECC technology such as hybrid fiber reinforcementand the material’s growing use in seismic structures. The paper also addresses the primary obstacles, including high initial costs and the absence of standardized specifications, while proposing future research paths aimed at optimizing ECC’s efficiency and economic viability.
Related References:
1. Singh, M.; Saini, B.; and Chalak, H. D., “Performance and Composition Analysis of Engineered Cementitious Composite (ECC): A Review,” Journal of Building Engineering, V. 26, 2019, pp. 1-8. doi: 10.1016/j.jobe.2019.100851
2. Li, V. C., “On Engineered Cementitious Composites (ECC): A Review of the Material and its Applications,” Journal of Advanced Concrete Technology, V. 1, No. 3, 2003, pp. 215-230. doi: 10.3151/jact.1.215
3. Li, V. C., Engineered Cementitious Composites (ECC): Bendable Concrete for Sustainable and Resilient Infrastructure, Springer, Berlin, Germany, 2019.
4. Bentur, A., and Mindess, S., Fibre Reinforced Cementitious Composites, second edition, E & FN Spon, London, UK, 2007.
5. Hajj, E.; Sanders, D. H.; and Weitzel, N. D., “Development of Specifications for Engineered Cementitious Composites for Use in Bridge Deck Overlays,” University of Nevada, Reno, Reno, NV, 2016.
6. Park, P.; Jones, R.; Castillo, L.; Vallangca, M.; and Cantu, F., “Engineered Cementitious Composites (ECC) for Applications in Texas,” Technical Report 0-7030-1, TxDOT Project Number 0-7030, The University of Texas Rio Grande Valley, Edinburg, TX, 2020.
7. Barbhuiya, S.; Das, B. B.; and Adak, D., “Advances and Perspectives in Engineered Cementitious Composites (ECC): A Comprehensive Review,” Magazine of Concrete Research, V. 76, No. 20, 2024, pp. 1165-1184. doi: 10.1680/jmacr.24.00047
8. Deng, B. Y.; Li, L. Z.; Tan, D.; Uddin, M. N.; Cai, Z. W.; and Yu, K. Q., “Sustainable and Cost-Effective Ultra-Lightweight Engineered Cementitious Composite: Design and Material Characterization,” Cement and Concrete Composites, V. 136, 2023, p. 104895. doi: 10.1016/j.cemconcomp.2022.104895
9. Liao, Q.; Su, Y. R.; Yu, J. T.; and Yu, K. Q., “Compression-Shear Performance and Failure Criteria of Seawater Sea-Sand Engineered Cementitious Composites with Polyethylene Fibers,” Construction and Building Materials, V. 345, 2022, p. 128386. doi: 10.1016/j.conbuildmat.2022.128386
10. Billington, S. L., and Yoon, J. K., “Cyclic Response of Unbonded Posttensioned Precast Columns with Ductile Fiber-Reinforced Concrete,” Journal of Bridge Engineering, ASCE, V. 9, No. 4, 2004, pp. 353-363. doi: 10.1061/(ASCE)1084-0702(2004)9:4(353)
11. Meng, D.; Huang, T.; Zhang, Y. X.; and Lee, C. K., “Mechanical Behaviour of a Polyvinyl Alcohol Fibre Reinforced Engineered Cementitious Composite (PVA-ECC) Using Local Ingredients,” Construction and Building Materials, V. 141, 2017, pp. 259-270. doi: 10.1016/j.conbuildmat.2017.02.158
12. Li, J., and Yang, E. H., “Macroscopic and Micro Structural Properties of Engineered Cementitious Composites Incorporating Recycled Concrete Fines,” Cement and Concrete Composites, V. 78, 2017, pp. 33-42. doi: 10.1016/j.cemconcomp.2016.12.013
13. Huang, T., and Zhang, Y. X., “Mechanical Properties of a PVA Fiber Reinforced Engineered Cementitious Composites,” Sustainable Solutions in Structural Engineering and Construction, 2014, pp. 439-444.
14. Zhou, J.; Quian, S.; and Breugel, K. V., “Engineered Cementitious Composites with Low Volume of Cementitious Materials,” Fracture Mechanics of Concrete and Concrete Structures: Proceedings of FraMCoS-7, 2010 May 23-28, 2010, pp. 1551-1556.
15. Huang, B. T.; Weng, K. F.; Zhu, J. X.; Xiang, Y.; Dai, J. G.; and Li, V. C., “Engineered/Strain-Hardening Cementitious Composites (ECC/SHCC) with an Ultra-High Compressive Strength over 210 MPa,” Composites Communications, V. 26, 2021, p. 100775. doi: 10.1016/j.coco.2021.100775
16. Zhou, J.; Pan, J.; and Leung, C. K., “Mechanical Behavior of Fiber-Reinforced Engineered Cementitious Composites in Uniaxial Compression,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 1, 2015, p. 04014111. doi: 10.1061/(ASCE)MT.1943-5533.0001034
17. Huang, X.; Ranade, R.; Zhang, Q.; Ni, W.; and Li, V. C., “Mechanical and Thermal Properties of Green Lightweight Engineered Cementitious Composites,” Construction and Building Materials, V. 48, 2013, pp. 954-960. doi: 10.1016/j.conbuildmat.2013.07.104
18. Wang, S. X., and Li, V. C., “Polyvinyl Alcohol Fiber Reinforced Engineered Cementitious Composites: Materials Design and Performances,” International RILEM Workshop on High Performance Fiber Reinforced Cementitious Composites (HPFRCC) in Structural Applications, G. Fischer and V. C. Li, eds., Honolulu, HI, 2005, pp. 65-73.
19. Yu, K.; McGee, W.; Ng, T. Y.; Zhu, H.; and Li, V. C., “3D-Printable Engineered Cementitious Composites (3DP-ECC): Fresh and Hardened Properties,” Cement and Concrete Research, V. 143, 2021, p. 106388. doi: 10.1016/j.cemconres.2021.106388
20. Sahmaran, M.; Lachemi, M.; and Li, V. C., “Assessing Mechanical Properties and Microstructure of Fire-Damaged Engineered Cementitious Composites,” ACI Materials Journal, V. 107, No. 3, May-June 2010, pp. 297-304.
21. Yu, K. Q.; Yu, J. T.; Dai, J. G.; Lu, Z. D.; and Shah, S. P., “Development of Ultra-High Performance Engineered Cementitious Composites Using Polyethylene (PE) Fibers,” Construction and Building Materials, V. 158, 2018, pp. 217-227. doi: 10.1016/j.conbuildmat.2017.10.040
22. Li, V., “Tailoring ECC for Special Attributes: A Review,” International Journal of Concrete Structures and Materials, V. 6, No. 3, 2012, pp. 135-144. doi: 10.1007/s40069-012-0018-8
23. Zhou, Y. W.; Xi, B.; Yu, K. Q.; Sui, L. L.; and Xing, F., “Mechanical Properties of Hybrid Ultra-High Performance Engineered Cementitious Composites Incorporating Steel and Polyethylene Fibers,” Materials, V. 11, No. 8, 2018, p. 1448. doi: 10.3390/ma11081448
24. Ajith, G.; Shanmugasundaram, N.; and Praveenkumar, S., “Effect of Mineral Admixtures and Manufactured Sand on Compressive Strength of Engineered Cementitious Composite,” Journal of Building Pathology and Rehabilitation, V. 6, No. 1, 2021, p. 38. doi: 10.1007/s41024-021-00137-y
25. Altwair, N. M.; Magat Johari, M. A.; and Saiyid Hashim, S. F., “Flexural Performance of Green Engineered Cementitious Composites Containing High Volume of Palm Oil Fuel Ash,” Construction and Building Materials, V. 37, 2012, pp. 518-525. doi: 10.1016/j.conbuildmat.2012.08.003
26. Zhu, J. X.; Xu, L. Y.; Huang, B. T.; Weng, K. F.; and Dai, J. G., “Recent Developments in Engineered/Strain-Hardening Cementitious Composites (ECC/SHCC) with High & Ultra-High Strength,” Construction and Building Materials, V. 342, 2022, p. 127956. doi: 10.1016/j.conbuildmat.2022.127956
27. Zhang, Z., and Qian, S., “Influence of Crumb Rubber on the Mechanical Behavior of Engineered Cementitious Composites,” VIII International Conference on Fracture Mechanics of Concrete and Concrete Structures FraMCOS-8, Toledo, Spain, 2013, pp. 1-10.
28. Ling, G.; Shui, Z.; Gao, X.; Sun, T.; Yu, R.; and Li, X., “Utilizing Iron Ore Tailing as Cementitious Material for Eco-Friendly Design of Ultra-High-Performance Concrete (UHPC),” Materials, V. 14, No. 8, 2021, p. 1829. doi: 10.3390/ma14081829
29. Gulghane, A. A., and Bari, C., “Comparative Analysis of ECC by Partial Replacement of Cement with Slag Sand,” Smart Technologies for Energy, Environment and Sustainable Development - Select Proceedings of ICSTEESD 2018, M. L. Kolhe, P. K. Labhasetwar, and H. M. Suryawanshi, eds., Springer, Singapore, 2019, pp. 427-435.
30. Turk, K., and Demirhan, S., “The Mechanical Properties of Engineered Cementitious Composites Containing Limestone Powder Replaced by Microsilica Sand,” Canadian Journal of Civil Engineering, V. 40, No. 2, 2013, pp. 151-157. doi: 10.1139/cjce-2012-0281
31. Raza, A.; Zhang, J.; Xu, S.; Umar, M.; and Yuan, C., “Experimental Analysis of Frost Resistance and Failure Models in Engineered Cementitious Composites with the Integration of Yellow River Sand,” Science and Engineering of Composite Materials, V. 31, No. 1, 2024, pp. 1-19. doi: 10.1515/secm-2024-0017
32. Lepech, M. D., and Li, V. C., “Water Permeability of Engineered Cementitious Composites,” Cement and Concrete Composites, V. 31, No. 10, 2009, pp. 744-753. doi: 10.1016/j.cemconcomp.2009.07.002
33. Maalej, M., and Li, V. C., “Introduction of Strain-Hardening Engineered Cementitious Composites in the Design of Reinforced Concrete Flexural Members for Improved Durability,” ACI Structural Journal, V. 92, No. 2, Mar.-Apr. 1995, pp. 167-176.
34. Li, V. C., “Engineered Cementitious Composites - Tailored Composites through Micromechanical Modeling,” Fiber Reinforced Concrete: Present and the Future, N. Banthia, A. Bentur, and A. Mufti, eds., Canadian Society for Civil Engineering, Montreal, QC, Canada, 1998, pp. 64-97.
35. Maalej, M.; Quek, S. T.; Ahmed, S. F. U.; Zhang, J.; Lin, V. W. J.; and Leong, K. S., “Review of Potential Structural Applications of Hybrid Fiber Engineered Cementitious Composites,” Construction and Building Materials, V. 36, 2012, pp. 216-227. doi: 10.1016/j.conbuildmat.2012.04.010
36. Soe, K. T.; Zhang, Y. X.; and Zhang, L. C., “Material Properties of a New Hybrid Fiber-Reinforced Engineered Cementitious Composite,” Construction and Building Materials, V. 43, 2013, pp. 399-407. doi: 10.1016/j.conbuildmat.2013.02.021
37. Kawamata, A.; Mihashi, H.; and Fukuyama, H., “Properties of Hybrid Fiber Reinforced Cement-Based Composites,” Journal of Advanced Concrete Technology, V. 1, No. 3, 2003, pp. 283-290. doi: 10.3151/jact.1.283
38. Lawler, J. S.; Zampini, D.; and Shah, S. P., “Micro Fiber and Macro Fiber Hybrid Fiber-Reinforced Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 17, No. 5, 2005, pp. 595-604. doi: 10.1061/(ASCE)0899-1561(2005)17:5(595)
39. AASHTO T 132-87(R2013), “Standard Method of Test for Tensile Strength of Hydraulic Cement Mortars,” American Association of State Highway and Transportation Officials, Washington, DC, 2013.
40. RILEM TC 162-TDF, “Uni-Axial Tension Test for Steel Fibre Reinforced Concrete,” Materials and Structures, V. 34, No. 1, 2001, pp. 3-6. doi: 10.1007/BF02482193
41. AFGC, Ultra-High-Performance Fibre-Reinforced Concretes—Interim Recommendations, AFGC Scientific and Technical Documents, Association Française de Génie Civil, Paris, France, 2002.
42. JSCE Concrete Committee, Recommendations for Design and Construction of High-Performance Fiber Reinforced Cement Composites with Multiple Fine Cracks (HPFRCC), Japan Society of Civil Engineers, Tokyo, Japan, 2008.
43. ASTM C293/C293M-10, “Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Center-Point Loading),” ASTM International, West Conshohocken, PA, 2010.
44. ASTM C78/C78M-10, “Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2010.
45. ASTM C1399/C1399M-10, “Standard Test Method for Obtaining Average Residual-Strength of Fiber-Reinforced Concrete,” ASTM International, West Conshohocken, PA, 2010.
46. ASTM C1609/C1609M-12, “Standard Test Method for Flexural Performance of Fiber-Reinforced Concrete (Using Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2012.
47. RILEM TC 162-TDF, “Test and Design Methods for Steel Fiber Reinforced Concrete: Bending Test,” Materials and Structures, V. 35, No. 9, 2002, pp. 579-582.
48. BS EN 14651:2005+A1:2007, “Test Method for Metallic Fibre Concrete: Measuring the Flexural Tensile Strength (Limit of Proportionality (LOP), Residual),” British Standards Institution, London, UK, 2007.
49. Zhang, D.; Yu, J.; Wu, H.; Jaworska, B.; Ellis, B. R.; and Li, V. C., “Discontinuous Micro-Fibers as Intrinsic Reinforcement for Ductile Engineered Cementitious Composites (ECC),” Composites Part B: Engineering, V. 184, 2020, p. 107741. doi: 10.1016/j.compositesb.2020.107741
50. Sun, R.; Hu, X.; Ling, Y.; Zuo, Z.; Zhuang, P.; and Wang, F., “Chloride Diffusion Behavior of Engineered Cementitious Composite under Dry-Wet Cycles,” Construction and Building Materials, V. 260, 2020, p. 119943. doi: 10.1016/j.conbuildmat.2020.119943
51. Li, M., and Li, V. C., “Cracking and Healing of Engineered Cementitious Composites under Chloride Environment,” ACI Materials Journal, V. 108, No. 3, May-June 2011, pp. 333-341.
52. Sun, R.; Lu, W.; Ma, C.; Tawfek, A. M.; Guan, Y.; Hu, X.; Zhang, H.; Ling, Y.; and Savija, B., “Effect of Crack Width and Wet-Dry Cycles on the Chloride Penetration Resistance of Engineered Cementitious Composite (ECC),” Construction and Building Materials, V. 352, 2022, p. 129030. doi: 10.1016/j.conbuildmat.2022.129030
53. Shumuye, E. D.; Li, W.; Liu, J.; Wang, Z.; Yu, J.; and Wu, H., “Self-Healing Recovery and Micro-Structural Properties of Slag/Fly-Ash Based Engineered Cementitious Composites under Chloride Environment and Tidal Exposure,” Cement and Concrete Composites, V. 134, 2022, p. 104789. doi: 10.1016/j.cemconcomp.2022.104789
54. Wang, L.; Han, X.; Tian, L.; Wang, P.; and Sun, X., “Influence of Frost Damage on Performance of Engineered Cementitious Composites,” Journal of Advanced Concrete Technology, V. 21, No. 12, 2023, pp. 971-982. doi: 10.3151/jact.21.971
55. Hou, L.; Xu, R.; Chen, D.; Xu, S.; and Aslani, F., “Seismic Behavior of Reinforced Engineered Cementitious Composite Members and Reinforced Concrete/Engineered Cementitious Composite Members: A Review,” Structural Concrete, V. 21, No. 1, 2020, pp. 199-219. doi: 10.1002/suco.201800269
56. Sasmal, S., and Avinash, G., “Investigations on Mechanical Performance of Cementitious Composites Micro-Engineered with Polyvinyl Alcohol Fibers,” Construction and Building Materials, V. 128, 2016, pp. 136-147. doi: 10.1016/j.conbuildmat.2016.10.025
57. Pan, Z.; Wu, C.; Liu, J.; Wang, W.; and Liu, J., “Study on Mechanical Properties of Cost-Effective Polyvinyl Alcohol Engineered Cementitious Composites (PVA-ECC),” Construction and Building Materials, V. 78, 2015, pp. 397-404. doi: 10.1016/j.conbuildmat.2014.12.071
58. Zhu, M.; Chen, B.; Wu, M.; and Han, J., “Effects of Different Mixing Ratio Parameters on Mechanical Properties of Cost-Effective Green Engineered Cementitious Composites (ECC),” Construction and Building Materials, V. 328, 2022, p. 127093. doi: 10.1016/j.conbuildmat.2022.127093
59. Yang, Y.; Gao, X.; Deng, H.; Yu, P.; and Yao, Y., “Effects of Water/Binder Ratio on the Properties of Engineered Cementitious Composites,” Journal of Wuhan University of Technology. Materials Science Edition, V. 25, No. 2, 2010, pp. 298-302. doi: 10.1007/s11595-010-2298-7
60. Şahmaran, M.; Bilici, Z.; Ozbay, E.; Erdem, T. K.; Yucel, H. E.; and Lachemi, M., “Improving the Workability and Rheological Properties of Engineered Cementitious Composites Using Factorial Experimental Design,” Composites Part B: Engineering, V. 45, No. 1, 2013, pp. 356-368. doi: 10.1016/j.compositesb.2012.08.015
61. Fischer, G., and Wang, S. X., “Design of Engineered Cementitious Composites (ECC) for Processing and Workability Requirements,” Brittle Matrix Composites 7, A. M. Brandt, V. C. Li, and I. H. Marshall, eds., Woodhead Publishing, Sawston, UK, 2003, pp. 29-36.
62. Kim, J. K.; Kim, J. S.; Ha, G. J.; and Kim, Y. Y., “Tensile and Fiber Dispersion Performance of ECC (Engineered Cementitious Composites) Produced with Ground Granulated Blast Furnace Slag,” Cement and Concrete Research, V. 37, No. 7, 2007, pp. 1096-1105. doi: 10.1016/j.cemconres.2007.04.006
63. Nicolaides, D.; Kanellopoulos, A.; Petrou, M.; Savva, P.; and Mina, A., “Development of a New Ultra-High-Performance Fiber Reinforced Cementitious Composite (UHPFRCC) for Impact and Blast Protection of Structures,” Construction and Building Materials, V. 95, 2015, pp. 667-674. doi: 10.1016/j.conbuildmat.2015.07.136
64. Ma, H.; Yi, C.; and Wu, C., “Review and Outlook on Durability of Engineered Cementitious Composite (ECC),” Construction and Building Materials, V. 287, 2021, p. 122719. doi: 10.1016/j.conbuildmat.2021.122719
65. Xu, S. L., and Cai, X. H., “Experimental Study of the Durability Properties of Ultra-High Toughness Cementitious Composites under Freeze and Thawing Cycles,” Tumu Gongcheng Xuebao, V. 42, No. 9, 2009, pp. 42-46.
66. Xu, S. L., and Cai, X. H., “Experimental Studies on Permeability and Carbonation Properties of Ultra-High Toughness Cementitious Composites,” Acta Materiae Compositae Sinica, V. 27, No. 3, 2010, pp. 177-183.
67. Ranjith, S.; Venkatasubramani, R.; and Sreevidya, V., “Comparative Study on Durability Properties of Engineered Cementitious Composites with Polypropylene Fiber and Glass Fiber,” Archives of Civil Engineering, V. 63, No. 4, 2017, pp. 83-101. doi: 10.1515/ace-2017-0042
68. Şahmaran, M.; Ozbay, E.; Yucel, H. E.; Lachemi, M.; and Li, V., “Effect of Fly Ash and PVA Fiber on Microstructural Damage and Residual Properties of Engineered Cementitious Composites Exposed to High Temperatures,” Journal of Materials in Civil Engineering, ASCE, V. 23, No. 12, 2011, pp. 1735-1745. doi: 10.1061/(ASCE)MT.1943-5533.0000335
69. Yu, J. T.; Lin, J. H.; Zhang, Z. G.; and Li, V., “Mechanical Performance of ECC with High-Volume Fly ash after Sub-Elevated Temperature,” Construction and Building Materials, V. 99, 2015, pp. 82-89. doi: 10.1016/j.conbuildmat.2015.09.002
70. Mechtcherine, V.; Silva, F. A.; Müller, S.; Jun, P.; and Filho, R. D. T., “Coupled Strain Rate and Temperature Effects on the Tensile Behavior of Strain-Hardening Cement-Based Composites (SHCC) with PVA Fibers,” Cement and Concrete Research, V. 42, No. 11, 2012, pp. 1417-1427. doi: 10.1016/j.cemconres.2012.08.011
71. Ranade, R.; Heard, W. F.; and Williams, B. A., “Multi-Scale Mechanical Performance of High Strength-High Ductility Concrete,” Dynamic Behavior of Materials, Volume 1 - Proceedings of the 2015 Annual Conference on Experimental and Applied Mechanics, B. Song, L. Lamberson, D. Casem, and J. Kimberley, eds., Springer, Cham, Switzerland, 2016, pp. 93-101.
72. Ding, Y.; Yu, K.; and Mao, W., “Compressive Performance of All-Grade Engineered Cementitious Composites: Experiment and Theoretical Model,” Construction and Building Materials, V. 244, 2020, p. 118357. doi: 10.1016/j.conbuildmat.2020.118357
73. Ran, H. Y.; Elchalakani, M.; Boussaid, F.; Yehia, S.; Sadakkathulla, M. A.; and Yang, B., “Development and Evaluation of Conductive Ultra-Lightweight Cementitious Composites for Smart and Sustainable Infrastructure Applications,” Construction and Building Materials, V. 375, 2023, p. 131017. doi: 10.1016/j.conbuildmat.2023.131017
74. Ran, H. Y.; Elchalakani, M.; Liu, H. Y.; Yehia, S.; and Yang, B., “Development and Characteristics of Multifunctional Ultra-Lightweight Engineered Cementitious Composites Incorporating Cenospheres and PE Fibre,” Cement and Concrete Composites, V. 140, 2023, p. 105084. doi: 10.1016/j.cemconcomp.2023.105084
75. Ran, H. Y.; Elchalakani, M.; Yehia, S.; Cai, J. M.; and Yang, B., “Self-Sensing High-Performance Ultra-Lightweight Engineered Cementitious Composites Using Calcined Petroleum Coke,” Journal of Cleaner Production, V. 418, 2023, p. 138241. doi: 10.1016/j.jclepro.2023.138241
76. Kanda, T.; Lin, Z.; and Li, V., “Tensile Stress-Strain Modeling of Pseudostrain Hardening Cementitious Composites,” Journal of Materials in Civil Engineering, ASCE, V. 12, No. 2, 2000, pp. 147-156. doi: 10.1061/(ASCE)0899-1561(2000)12:2(147)
77. Schröfl, C.; Mechtcherine, V.; Kaestner, A.; Vontobel, P.; Hovind, J.; and Lehmann, E., “Transport of Water through Strain-Hardening Cement-Based Composite (SHCC) Applied on Top of Cracked Reinforced Concrete Slabs with and without Hydrophobization of Cracks-Investigation by Neutron Radiography,” Construction and Building Materials, V. 76, No. 1, 2015, pp. 70-86. doi: 10.1016/j.conbuildmat.2014.11.062
78. Shabakhty, N.; Karimi, H. R.; and Bakhtiary, A. Y., “Statistical Evaluation of Fracture and Mechanical Performance of Engineered Cementitious Composites (ECC), Containing Different Percentages of Glass, Polypropylene, Polyvinyl-Alcohol Fibers, and Fly Ash,” Construction and Building Materials, V. 417, 2024, p. 135247. doi: 10.1016/j.conbuildmat.2024.135247
79. Shabakhty, N.; Karimi, H. R.; and Yeganeh Bakhtiary, A., “Effect of Short to Long Hybrid Elastic/Hyperelastic (Glass/PP) Fibers on High-Strength Engineered Cementitious Composites (ECC), Along with Presenting a Constitutive Model,” Journal of Building Engineering, V. 89, 2024, p. 109215. doi: 10.1016/j.jobe.2024.109215
80. Saljoughian, A.; Bahmani, H.; Ansari, Z.; Jafari, N.; and Mostofinejad, D., “An Eco-Friendly ECC with High Slag and Polypropylene Fiber Content for High-Tensile Strain Applications,” Journal of Building Engineering, V. 91, 2024, p. 109726. doi: 10.1016/j.jobe.2024.109726
81. Lee, B. Y.; Kim, J. K.; Kim, J. S.; and Kim, Y. Y., “Quantitative Evaluation Technique of Polyvinyl Alcohol (PVA) Fiber Dispersion in Engineered Cementitious Composites,” Cement and Concrete Composites, V. 31, No. 6, 2009, pp. 408-417. doi: 10.1016/j.cemconcomp.2009.04.002
82. Sherir, M. A.; Hossain, K. M.; and Lachemi, M., “Fracture Energy Characteristics of Engineered Cementitious Composites Incorporating Different Aggregates,” CSCE 2014 4th International Structural Specialty Conference, Halifax, NS, Canada, 2014.
83. Said, S. H.; Razak, H. A.; and Othman, I., “Strength and Deformation Characteristics of Engineered Cementitious Composite Slabs with Different Polymer Fibers,” Journal of Reinforced Plastics and Composites, V. 34, No. 23, 2015, pp. 1950-1962. doi: 10.1177/0731684415607393
84. Tian, H., and Zhang, Y. X., “Ageing Effect on Tensile and Shrinkage Behaviour of New Green Hybrid Fibre-Reinforced Cementitious Composites,” Cement and Concrete Composites, V. 75, 2017, pp. 38-50. doi: 10.1016/j.cemconcomp.2016.11.005
85. Tian, H.; Zhang, Y. X.; Ye, L.; and Yang, C., “Mechanical Behaviours of Green Hybrid Fibre-Reinforced Cementitious Composites,” Construction and Building Materials, V. 95, 2015, pp. 152-163. doi: 10.1016/j.conbuildmat.2015.07.143
86. Tian, H., and Zhang, Y. X., “The Influence of Bagasse Fibre and Fly Ash on the Long-Term Properties of Green Cementitious Composites,” Construction and Building Materials, V. 111, 2016, pp. 237-250. doi: 10.1016/j.conbuildmat.2016.02.103
87. Yang, E.-H., and Li, V. C., “Strain-Hardening Fiber Cement Optimization and Component Tailoring by Means of a Micromechanical Model,” Construction and Building Materials, V. 24, No. 2, 2010, pp. 130-139. doi: 10.1016/j.conbuildmat.2007.05.014
88. Pakravan, H. R.; Jamshidi, M.; and Latifi, M., “The Effect of Hybridization and Geometry of Polypropylene Fibers on Engineered Cementitious Composites Reinforced by Polyvinyl Alcohol Fibers,” Journal of Composite Materials, V. 50, No. 8, 2016, pp. 1007-1020. doi: 10.1177/0021998315586078
89. Alrefaei, Y.; Rahal, K.; and Maalej, M., “Shear Strength of Beams Made Using Hybrid Fiber-Engineered Cementitious Composites,” Journal of Structural Engineering, ASCE, V. 144, No. 1, 2018, p. 04017177. doi: 10.1061/(ASCE)ST.1943-541X.0001924
90. Gadhiya, S.; Patel, T. N.; and Shah, D., “Parametric Study on Flexural Strength of ECC,” International Journal of Science Research and Development, V. 3, No. 4, 2015, pp. 1494-1497.
91. Mohammed, B. S.; Khed, V. K. C.; and Liew, M. S., “Optimization of Hybrid Fibers in Engineered Cementitious Composites,” Construction and Building Materials, V. 190, 2018, pp. 24-37. doi: 10.1016/j.conbuildmat.2018.08.188
92. Ali, M. A. E. M.; Soliman, A. M.; and Nehdi, M. L., “Hybrid-Fiber Reinforced Engineered Cementitious Composite under Tensile and Impact Loading,” Materials & Design, V. 117, 2017, pp. 139-149. doi: 10.1016/j.matdes.2016.12.047
93. Said, S. H.; Razak, H. A.; and Othman, I., “Flexural Behavior of Engineered Cementitious Composite (ECC) Slabs with Polyvinyl Alcohol Fibers,” Construction and Building Materials, V. 75, 2015, pp. 176-188. doi: 10.1016/j.conbuildmat.2014.10.036
94. Keoleian, G. A.; Kendall, A.; Dettling, J. E.; Smith, V. M.; Chandler, R. F.; Lepech, M. D.; and Li, V. C., “Life Cycle Modeling of Concrete Bridge Design: Comparison of Engineered Cementitious Composite Link Slabs and Conventional Steel Expansion Joints,” Journal of Infrastructure Systems, ASCE, V. 11, No. 1, 2005, pp. 51-60. doi: 10.1061/(ASCE)1076-0342(2005)11:1(51)
95. Thaishnavi, A.; Suryaprakash, S.; and Krishnaraja, A. R., “Experimental Studies on Properties of Engineered Cementitious Composites,” South Asian Journal of Engineering and Technology, V. 2, No. 21, 2016, pp. 217-222.
96. Gencturk, B., and Hosseini, F., “Evaluation of Reinforced Concrete and Reinforced Engineered Cementitious Composites (ECC) Members and Structures Using Small-Scale Testing,” Canadian Journal of Civil Engineering, V. 42, No. 3, 2015, pp. 164-177. doi: 10.1139/cjce-2013-0445
97. Wang, Q.; Yi, Y.; Ma, G.; and Luo, H., “Hybrid Effects of Steel Fibers, Basalt Fibers and Calcium Sulfate on Mechanical Performance of PVA-ECC Containing High-Volume Fly Ash,” Cement and Concrete Composites, V. 97, 2019, pp. 357-368. doi: 10.1016/j.cemconcomp.2019.01.009
98. Al-Gemeel, A. N.; Zhuge, Y.; and Youssf, O., “Experimental Investigation of Basalt Textile Reinforced Engineered Cementitious Composite under Apparent Hoop Tensile Loading,” Journal of Building Engineering, V. 23, 2019, pp. 270-279. doi: 10.1016/j.jobe.2019.01.037
99. Felekoglu, B.; Tosun-Felekoglu, K.; Ranade, R.; Zhang, Q.; and Li, V. C., “Influence of Matrix Flowability, Fiber Mixing Procedure, and Curing Conditions on the Mechanical Performance of HTPP-ECC,” Composites Part B: Engineering, V. 60, 2014, pp. 359-370. doi: 10.1016/j.compositesb.2013.12.076
100. Afefy, H. M. E. D., and Mahmoud, M. H., “Structural Performance of RC Slabs Provided by Pre-Cast ECC Strips in Tension Cover Zone,” Construction and Building Materials, V. 65, No. 29, 2014, pp. 103-113. doi: 10.1016/j.conbuildmat.2014.04.096
101. Maalej, M.; Quek, S. T.; and Zhang, J., “Behavior of Hybrid-Fiber Engineered Cementitious Composites Subjected to Dynamic Tensile Loading and Projectile Impact,” Journal of Materials in Civil Engineering, ASCE, V. 17, No. 2, 2005, pp. 143-152. doi: 10.1061/(ASCE)0899-1561(2005)17:2(143)
102. Fischer, G.; Fukuyama, H.; and Li, V. C., “Effect of Matrix Ductility on the Performance of Reinforced ECC Column Members under Reversed Cyclic Loading Conditions,” Proceedings of the DFRCC International Workshop, Takayama, Japan, 2002, pp. 269-278.
103. Yu, K.; Wang, Y.; Yu, J.; and Xu, S., “A Strain-Hardening Cementitious Composites with the Tensile Capacity Up to 8%,” Construction and Building Materials, V. 137, 2017, pp. 410-419. doi: 10.1016/j.conbuildmat.2017.01.060
104. Singh, S. B.; Munjal, P.; and Thammishetti, N., “Strengthening of Masonry Beam with ECC as Bed Joint,” Journal of Engineering Science and Technology, V. 10, 2015, pp. 29-39.
105. Qiu, J., and Yang, E. H., “Micromechanics-Based Investigation of Fatigue Deterioration of Engineered Cementitious Composite (ECC),” Cement and Concrete Research, V. 95, 2017, pp. 65-74. doi: 10.1016/j.cemconres.2017.02.029
106. Radhakrishnan, N.; Chellapandian, M.; and Singh, S. B., “Engineering Characteristics, Techno-Economic Feasibility and Life Cycle Assessment of Bio-Fiber Based Green Engineered Cementitious Composites,” Journal of Building Engineering, V. 96, 2024, p. 110521. doi: 10.1016/j.jobe.2024.110521
107. Tian, J.; Zhu, W.; Wu, X.; Yuan, J.; Zheng, Y.; Wang, W.-W.; Wei, L.; Zhang, W.; and Zheng, M., “Investigation on Shear Performance and Prediction Model of CFRP-ECC-Concrete Composite Interface Suffered from Anodic Polarization and Environmental Degradation,” Developments in the Built Environment, V. 18, 2024, p. 100422. doi: 10.1016/j.dibe.2024.100422
108. Ge, Z.; Tawfek, A. M.; Zhang, H.; Yang, Y.; Yuan, H.; Sun, R.; and Wang, Z., “Influence of an Extrusion Approach on the Fiber Orientation and Mechanical Properties of Engineered Cementitious Composite,” Construction and Building Materials, V. 306, 2021, p. 124876. doi: 10.1016/j.conbuildmat.2021.124876
109. Wang, Z.; Wang, P.; and Zhu, F., “Synergy Effect of Hybrid Steel-Polyvinyl Alcohol Fibers in Engineered Cementitious Composites: Fiber Distribution and Mechanical Performance,” Journal of Building Engineering, V. 62, 2022, p. 105348. doi: 10.1016/j.jobe.2022.105348
110. Lu, C., and Leung, C. K. Y., “Theoretical Evaluation of Fiber Orientation and its Effects on Mechanical Properties in Engineered Cementitious Composites (ECC) with Various Thicknesses,” Cement and Concrete Research, V. 95, 2017, pp. 240-246. doi: 10.1016/j.cemconres.2017.02.024
111. Pang, Z.; Lu, C.; Li, B.; and Wang, J., “A Multiscale Model for Quantifying Fiber Orientation Effects on the Tensile Properties of 3D Printed Engineered Cementitious Composites (3DP-ECC),” Journal of Building Engineering, V. 68, 2023, p. 106090. doi: 10.1016/j.jobe.2023.106090
112. Dong, B.; Liu, C.; Shumuye, E. D.; Zhang, Y.; Zhong, H.; and Fang, G., “Effect of Nano-Silica on Mechanical Properties and Microstructure of Engineered Geopolymer Composites,” Cement and Concrete Composites, V. 156, 2025, p. 105849. doi: 10.1016/j.cemconcomp.2024.105849
113. Li, V. C.; Mishra, D. K.; Naaman, A. E.; Wight, J. K.; LaFave, J. M.; Wu, H. C.; and Inada, Y., “On the Shear Behavior of Engineered Cementitious Composites,” Advanced Cement Based Materials, V. 1, No. 3, 1994, pp. 142-149. doi: 10.1016/1065-7355(94)90045-0
114. Li, V. C., and Wang, S., “Failure Mode and Structural Ductility of GFRP Reinforced Engineered Cementitious Composite Beams,” ACI Materials Journal, V. 99, No. 1, Jan.-Feb. 2002, pp. 11-21.
115. Yuan, F.; Pan, J.; Dong, L.; and Leung, C. K. Y., “Mechanical Behaviors of Steel Reinforced ECC or ECC/Concrete Composite Beams under Reversed Cyclic Loading,” Journal of Materials in Civil Engineering, ASCE V. 26, No. 8, 2014, p. 04014047. doi: 10.1061/(ASCE)MT.1943-5533.0000935
116. Zhu, H.; Zhang, D.; Wang, T.; McBain, M.; and Li, V. C., “Intrinsic Self-Stressing and Low Carbon Engineered Cementitious Composites (ECC) for Improved Sustainability,” Cement and Concrete Research, V. 149, 2021, p. 106580. doi: 10.1016/j.cemconres.2021.106580
117. Zhang, Z.; Liu, S.; Yang, F.; Weng, Y.; and Qian, S., “Sustainable High Strength, High Ductility Engineered Cementitious Composites (ECC) with Substitution of Cement by Rice Husk Ash,” Journal of Cleaner Production, V. 317, 2021, p. 128379. doi: 10.1016/j.jclepro.2021.128379
118. Larson, M. B., “Bridge Decks Going Jointless: Cementitious Composites Improve Durability of Link Slabs,” Construction and Technology Research Record, V. 100, 2005, pp. 342-348.
119. Kim, Y. Y.; Fischer, G.; and Li, V. C., “Performance of Bridge Deck Link Slabs Designed with Ductile Engineered Cementitious Composites,” ACI Structural Journal, V. 101, No. 6, Nov.-Dec. 2004, pp. 792-801.
120. Fischer, G., and Li, V. C., “Deformation Behavior of Fiber-Reinforced Polymer Reinforced Engineered Cementitious Composite (ECC) Flexural Members under Reversed Cyclic Loading Conditions,” ACI Structural Journal, V. 100, No. 1, Jan.-Feb. 2003, pp. 25-34.
121. Kanda, T.; Watanabe, S.; and Li, V. C., “Application of Pseudo Strain Hardening Cementitious Composites to Shear Resistant Structural Elements,” Fracture Mechanics of Concrete Structures, Proceedings FRAMCOS-3, AEDIFICATIO Publishers, Freiburg, Germany, 1998, pp. 1477-1490.
122. Krouma, A., and Syed, Z. I., “A Review on the Use of Engineered Cementitious Composite in Bridges,” Materials Science Forum, V. 860, No. 1, 2016, pp. 125-134. doi: 10.4028/www.scientific.net/MSF.860.125
123. Lepech, M., and Li, V. C., “Sustainable Pavement Overlays Using Engineered Cementitious Composites,” International Journal of Pavement Research and Technology, V. 3, No. 5, 2010, pp. 241-250.
124. Mishra, D. K.; Ranjan, P.; Sun, H.; Yu, J.; and Ng, P. L., “Applications of Drone Inspection and Use of Strain-Hardening Cementitious Composites (ECC/SHCC) in Lowering Carbon Footprint and Lifecycle Cost of Bridges,” Life-Cycle of Structures and Infrastructure Systems, 2023, pp. 4029-4036.
125. Li, V. C., and Kanda, T., “INNOVATIONS FORUM: Engineered Cementitious Composites for Structural Applications,” Journal of Materials in Civil Engineering, ASCE, V. 10, No. 2, 1998, pp. 66-69. doi: 10.1061/(ASCE)0899-1561(1998)10:2(66)
126. Singh, S. B., and Munjal, P., “Engineered Cementitious Composite and its Applications,” Materials Today: Proceedings, V. 32, No. 4, 2020, pp. 797-802. doi: 10.1016/j.matpr.2020.03.743
127. Şahmaran, M., and Li, V. C., “Durability of Mechanically Loaded Engineered Cementitious Composites under Highly Alkaline Environments,” Cement and Concrete Composites, V. 30, No. 2, 2008, pp. 72-81. doi: 10.1016/j.cemconcomp.2007.09.004
128. Shanmugasundaram, N., and Praveenkumar, S., “Mechanical Properties of Engineered Cementitious Composites (ECC) Incorporating Different Mineral Admixtures and Fibre: A Review,” Journal of Building Pathology and Rehabilitation, V. 7, No. 1, 2022, p. 40. doi: 10.1007/s41024-022-00182-1
129. Li, V. C., “Large Volume, High-Performance Applications of Fibers in Civil Engineering,” Journal of Applied Polymer Science, V. 83, No. 3, 2002, pp. 660-686. doi: 10.1002/app.2263
130. Arce, G.; Noorvand, H.; Hassan, M.; Rupnow, T.; and Hungria, R., “Cost-Effective ECC with Low Fiber Content for Pavement Application,” MATEC Web of Conferences, V. 271, 2019, p. 07001.
131. Arce, G.; Rupnow, T.; and Hassan, M., “Evaluation of the Performance and Cost-Effectiveness of Engineered Cementitious Composites (ECC) Produced from Region 6 Local Materials,” Project No. 17CLSU05, Transportation Consortium of South-Central States (Tran-SET), Louisiana State University, Baton Rouge, LA, 2018.