Cyclic Loading Test for Precast Columns Using Slag-Based Concrete and Sleeve Splices

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cyclic Loading Test for Precast Columns Using Slag-Based Concrete and Sleeve Splices

Author(s): H.-S. Moon, K.-W. Jo, H.-J. Hwang, C.-S. Kim, J.-H. Jeong, C.-K. Park, and H.-G. Park

Publication: Structural Journal

Volume: 122

Issue: 5

Appears on pages(s): 45-55

Keywords: column; cyclic loading test; precast concrete; seismic performance; slag-based concrete; sleeve splice; zero-cement concrete

DOI: 10.14359/51746791

Date: 9/1/2025

Abstract:
Slag-based zero-cement concrete (ZC) of high strength (60 MPa [8.70 ksi]) was developed as an eco-friendly construction material. In the present study, to investigate the structural behavior of precast columns using ZC, cyclic loading tests were performed for five column specimens with reinforcement details of ordinary moment frames. Longitudinal reinforcement was connected by sleeve splices at the precast column-footing joint. The test parameters included the concrete type (portland cement-based normal concrete [NC] versus ZC), construction method (monolithic versus precast), longitudinal reinforcement ratio, and sleeve size. The test results showed that the structural performance (failure mode, strength, stiffness, energy dissipation, and deformation capacity) of the precast ZC columns was comparable to that of the monolithic NC and precast NC columns, and the tested strengths agreed with the nominal strengths calculated by ACI 318-19. These results indicate that current design codes for cementitious materials and sleeve splice of longitudinal reinforcement are applicable to the design of precast ZC columns.

Related References:

1. Mo, K. H.; Alengaram, U. J.; and Jumaat, M. Z., “Structural Performance of Reinforced Geopolymer Concrete Members: A Review,” Construction and Building Materials, V. 120, May 2016, pp. 251-264. doi: 10.1016/j.conbuildmat.2016.05.088

2. Vashistha, P.; Park, S.; and Pyo, S., “A Review on Sustainable Fabrication of Futuristic Cementitious Binders based on Application of Waste Concrete Powder, Steel Slags, and Coal Bottom Ash,” International Journal of Concrete Structures and Materials, V. 16, No. 1, 2022, pp. 1-28. doi: 10.1186/s40069-022-00541-9

3. Bakhoum, E. S., and Mater, Y. M., “Decision Analysis for the Influence of Incorporating Waste Materials on Green Concrete Properties,” International Journal of Concrete Structures and Materials, V. 16, No. 1, 2022, pp. 1-16. doi: 10.1186/s40069-022-00553-5

4. Aldred, J., and Day, J., “Is Geopolymer Concrete a Suitable Alternative to Traditional Concrete?” Proceedings of the 37th Conference on Our World in Concrete & Structures, Singapore, Aug. 2012, pp. 29-31.

5. Srividya, T.; PR, K. R.; Sivasakthi, M.; Sujitha, A.; and Jeyalakshmi, R., “A State-of-the-Art on Development of Geopolymer Concrete and Its Field Applications,” Case Studies in Construction Materials, V. 16, June 2022, p. e00812.

6. Ma, C. K.; Awang, A. Z.; and Omar, W., “Structural and Material Performance of Geopolymer Concrete: A Review,” Construction and Building Materials, V. 186, Oct. 2018, pp. 90-102. doi: 10.1016/j.conbuildmat.2018.07.111

7. Amran, Y. M.; Alyousef, R.; Alabduljabbar, H.; and El-Zeadani, M., “Clean Production and Properties of Geopolymer Concrete; A Review,” Journal of Cleaner Production, V. 251, Apr. 2020, p. 119679. doi: 10.1016/j.jclepro.2019.119679

8. Patil, A. A.; Chore, H.; and Dodeb, P., “Effect of Curing Condition on Strength of Geopolymer Concrete,” Advances in Concrete Construction, V. 2, No. 1, 2014, pp. 29-37. doi: 10.12989/acc.2014.2.1.029

9. Du, Y.; Wang, J.; Shi, C.; Hwang, H. J.; and Li, N., “Flexural Behavior of Alkali-Activated Slag-based Concrete Beams,” Engineering Structures, V. 229, Feb. 2021, p. 111644. doi: 10.1016/j.engstruct.2020.111644

10. Shibayama, A., and Nishiyama, M., “Flexural Strength and Load−Deformation Relationship of Fly-Ash Based Geopolymer Concrete Beams,” Japan Architectural Review, V. 6, No. 1, 2023, p. e12331. doi: 10.1002/2475-8876.12331

11. Alex, A. G.; Gebrehiwet Tewele, T.; Kemal, Z.; and Subramanian, R. B., “Flexural Behavior of Low Calcium Fly Ash Based Geopolymer Reinforced Concrete Beam,” International Journal of Concrete Structures and Materials, V. 16, No. 1, 2022, p. 40. doi: 10.1186/s40069-022-00531-x

12. Wu, C.; Hwang, H. J.; Shi, C.; Li, N.; and Du, Y., “Shear Tests on Reinforced Slag-Based Geopolymer Concrete Beams with Transverse Reinforcement,” Engineering Structures, V. 219, Sept. 2020, p. 110966. doi: 10.1016/j.engstruct.2020.110966

13. Saranya, P.; Nagarajan, P.; and Shashikala, A. P., “Behaviour of GGBS-Dolomite Geopolymer Concrete Short Column Under Axial Loading,” Journal of Building Engineering, V. 30, July 2020, p. 101232. doi: 10.1016/j.jobe.2020.101232

14. Ganesan, N.; Indira, P. V.; and Santhakumar, A., “Prediction of Ultimate Strength of Reinforced Geopolymer Concrete Wall Panels in One-Way Action,” Construction and Building Materials, V. 48, Nov, 2013, pp. 91-97. doi: 10.1016/j.conbuildmat.2013.06.090

15. Cárdenas-Pulido, J.; Reyes, J. C.; Carrillo, J.; and Ramírez, F., “Shear Behavior of Geopolymer Concrete Panels Under Diagonal Tensile Stresses,” Engineering Structures, V. 212, June 2020, p. 110518. doi: 10.1016/j.engstruct.2020.110518

16. Huang, J. Q.; Kumar, S.; and Dai, J. G., “Flexural Performance of Steel-Reinforced Geopolymer Concrete One-Way Slabs: Experimental and Numerical Investigations,” Construction and Building Materials, V. 366, Feb. 2023, p. 130098. doi: 10.1016/j.conbuildmat.2022.130098

17. Mohmmad, S. H.; Gülşan, M. E.; and Çevik, A., “Punching Shear Behaviour of Geopolymer Concrete Two-Way Slabs Reinforced by FRP Bars Under Monotonic and Cyclic Loadings,” Advances in Structural Engineering, V. 25, No. 3, 2022, pp. 453-472. doi: 10.1177/13694332211052349

18. Chen, C.; Zhang, X.; and Hao, H., “Investigation on The Impact Resistance of Reinforced Geopolymer Concrete Slab,” Journal of Cleaner Production, V. 406, June 2023, p. 137144. doi: 10.1016/j.jclepro.2023.137144

19. Zhang, H. Y.; Kodur, V.; Wu, B.; Yan, J.; and Yuan, Z. S., “Effect of Temperature on Bond Characteristics of Geopolymer Concrete,” Construction and Building Materials, V. 163, Feb. 2018, pp. 277-285. doi: 10.1016/j.conbuildmat.2017.12.043

20. Mao, Y.; Hwang, H. J.; Du, Y.; Su, J.; Hu, X.; Liu, Y.; and Shi, C., “Bond and Anchorage Performance of Beam Flexural Bars on Beam−Column Joints Using Slag-based Geopolymer Concrete and Their Effect on Seismic Performance,” Engineering Structures, V. 273, Dec. 2022, p. 115062. doi: 10.1016/j.engstruct.2022.115062

21. Mao, Y.; Du, Y.; Hwang, H. J.; Su, J.; Hu, X.; Liu, Y.; and Shi, C., “Seismic Performance of Interior Beam−Column Joints Using Reinforced Slag‐Based Geopolymer Concrete,” Earthquake Engineering & Structural Dynamics, V. 52, No. 2, 2023, pp. 285-307. doi: 10.1002/eqe.3760

22. Ngo, T. T.; Tran, T. T.; Pham, T. M.; and Hao, H., “Performance of Geopolymer Concrete in Monolithic and Non-Corrosive Dry Joints Using CFRP Bolts Under Cyclic Loading,” Composite Structures, V. 258, Feb. 2021, p. 113394. doi: 10.1016/j.compstruct.2020.113394

23. Saranya, P.; Nagarajan, P.; and Shashikala, A. P., “Seismic Performance of Geopolymer Concrete Beam−Column Joints Under Reverse Cyclic Loading,” Innovative Infrastructure Solutions, V. 6, No. 2, June 2021, pp. 1-10. doi: 10.1007/s41062-021-00474-4

24. Haber, Z. B.; Saiidi, M. S.; and Sanders, D. H., “Seismic Performance of Precast Columns with Mechanically Spliced Column−Footing Connections,” ACI Structural Journal, V. 111, No. 3, May-June 2014, pp. 639-650. doi: 10.14359/51686624

25. Ameli, M.; Parks, J. E.; Brown, D. N.; and Pantelides, C. P., “Seismic Evaluation of Grouted Splice Sleeve Connections for Reinforced Precast Concrete Column-To-Cap Beam Joints in Accelerated Bridge Construction,” PCI Journal, V. 60, No. 2, 2015, pp. 80-103. doi: 10.15554/pcij.03012015.80.103

26. Ameli, M. J.; Brown, D. N.; Parks, J. E.; and Pantelides, C. P., “Seismic Column-to-Footing Connections Using Grouted Splice Sleeves,” ACI Structural Journal, V. 113, No. 5, Sept.-Oct. 2016, pp. 1021-1030. doi: 10.14359/51688755

27. Qu, H.; Fu, J.; Li, T.; Wu, C.; Sun, X.; Wei, H.; and Wang, Z., “Experimental and Numerical Assessment of Precast Bridge Columns with Different Grouted Splice Sleeve Coupler Designs Based on Shake Table Test,” Journal of Bridge Engineering, ASCE, V. 26, No. 8, 2021, p. 04021055. doi: 10.1061/(ASCE)BE.1943-5592.0001748

28. Xin, G.; Xu, W.; Wang, J.; Yan, X.; Chen, Y.; Yan, W.; and Li, J., “Seismic Performance of Fabricated Concrete Piers with Grouted Sleeve Joints and Bearing-Capacity Estimation Method,” Structures, V. 33, Apr. 2021, pp. 169-186. doi: 10.1016/j.istruc.2021.04.047

29. Xiao, S.; Wang, Z.; Li, X.; Harries, K. A.; Xu, Q.; and Gao, R., “Study of Effects of Sleeve Grouting Defects on the Seismic Performance of Precast Concrete Shear Walls,” Engineering Structures, V. 236, June 2021, p. 111833. doi: 10.1016/j.engstruct.2020.111833

30. Xie, L.; Wang, X.; Zhong, B.; Yang, C.; Chen, X.; Miao, Q.; and Liu, Q., “Full-Scale Experimental Investigation on the Seismic Performance of PC Columns Before and After Repair of Grouting Defects,” Journal of Building Engineering, V. 58, Oct. 2022, p. 104996. doi: 10.1016/j.jobe.2022.104996

31. ACI Committee 374, “Acceptance Criteria for Moment Frames Based on Structural Testing and Commentary (ACI 374.1-05),” American Concrete Institute, Farmington Hills, MI, 2005, 9 pp.

32. AIJ, “Guidelines for the Design of Structural Precast Concrete Emulating Cast-in-Place Reinforced Concrete (AIJ Guidelines),” Architectural Institute of Japan, Tokyo, Japan, 2002.

33. Korean Standards Information Center, “Hydraulic-Cement Grout (Nonshrink) (KS F 4044),” Chungcheongbuk-do, Republic of Korea, 2019.

34. Park, R., “Evaluation of Ductility of Structures and Structural Assemblages from Laboratory Testing,” Bulletin of the New Zealand Society for Earthquake Engineering, V. 22, No. 3, 1989, pp. 155-166. doi: 10.5459/bnzsee.22.3.155-166

35. Joint ACI-ASCE Committee 352, “Recommendations for Design of Beam-Column Connections in Monolithic Reinforced Concrete Structures (ACI 352R-02),” American Concrete Institute, Farmington Hills, MI, 2002, 38 pp.

36. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” Farmington Hills, MI, American Concrete Institute, 2019, 624 pp.


ALSO AVAILABLE IN: